Roll material for manufacturing electromagnetic induction sealing liner and sealing liner
US-2024424770-A1 · Dec 26, 2024 · US
US9789670B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9789670-B2 |
| Application number | US-201013388350-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 11, 2010 |
| Priority date | Aug 11, 2009 |
| Publication date | Oct 17, 2017 |
| Grant date | Oct 17, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
[Problems to be Solved] To coat homopolyethylene terephthalate, which is inexpensive and easily available, on a paper base material directly, not via an adhesive layer, by extrusion coating, thereby providing a paper laminate having heat sealability and having a homopolyethylene terephthalate coating of a uniform film thickness formed thereon. [Means to Solve the Problems] A method for producing a paper laminate having a coating comprising homopolyethylene terephthalate formed on at least one surface of a paper base material by extrusion coating is characterized in that an air gap L, expressed as a distance from a lip opening of a T-die to a paper base material B, is 25 cm or less.
Opening claim text (preview).
The invention claimed is: 1. A method for producing, by an extrusion coating method, a heat-sealable laminate by directly applying a heat-sealable coating composed of a homopolyethylene terephthalate onto the surface of a paper substrate or onto the surface of an aluminum foil laminated on the surface of the paper substrate, wherein said homopolyethylene terephthalate has an intrinsic viscosity in a range of from 0.72 to 0.88 dl/g, the temperature of the homopolyethylene terephthalate when it is melt-extruded by the extrusion-coating method is in a range of from Tm+25° C. to Tm+60° C. based on a melting point (Tm) of said homopolyethylene terephthalate, the extrusion pressure is in a range of from 4.0 to 6.0 MPa, and an air gap, expressed as a distance of from a lip opening of a T-die to the surface of the paper substrate or to the surface of the aluminum foil, is 25 cm or less, and a thickness of the homopolyethylene terephthalate coating varies in a range of less than ±20%.
of paper or cardboard · CPC title
Synthetic resin or polymer · CPC title
comprising polyesters · CPC title
Layered products comprising {a layer of} paper or cardboard · CPC title
Paper containing [e.g., paperboard, cardboard, fiberboard, etc.] · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.