Sintered body production method
US-2024307956-A1 · Sep 19, 2024 · US
US9789544B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9789544-B2 |
| Application number | US-201414295395-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 4, 2014 |
| Priority date | Feb 9, 2006 |
| Publication date | Oct 17, 2017 |
| Grant date | Oct 17, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of making a degradable alloy includes adding one or more alloying products to an aluminum or aluminum alloy melt; dissolving the alloying products in the aluminum or aluminum alloy melt, thereby forming a degradable alloy melt; and solidifying the degradable alloy melt to form the degradable alloy. A method for manufacturing a product made of a degradable alloy includes adding one or more alloying products to an aluminum or aluminum alloy melt in a mold; dissolving the one or more alloying products in the aluminum or aluminum alloy melt to form a degradable alloy melt; and solidifying the degradable alloy melt to form the product. A method for manufacturing a product made of a degradable alloy includes placing powders of a base metal or a base alloy and powders of one or more alloying products in a mold; and pressing and sintering the powders to form the product.
Opening claim text (preview).
What is claimed is: 1. A method for manufacturing a degradable gun carrier, comprising: placing powders of a base metal or a base alloy and powders of one or more alloying elements selected from the group consisting of as gallium, indium, zinc, and bismuth in a gun carrier tubing mould, wherein the base metal or the base alloy is aluminum or aluminum alloy; and pressing and sintering the powders to form the gun carrier. 2. The method of claim 1 , wherein the powders of the base metal or the base alloy and the powders of the one or more alloying elements are pre-mixed before the placing in the mould. 3. The method of claim 1 , further comprising placing powders of a non-metallic material in the mould before the placing and the sintering. 4. The method of claim 3 , wherein the non-metallic material comprises ceramics. 5. The method of claim 1 , wherein the powders of the one or more alloying elements is selected because it will render the gun carrier degradable in water. 6. The method of claim 1 , wherein the powders of the one or more alloying elements is selected because it will render the gun carrier degradable in fluid having a pH greater than 7.0. 7. The method of claim 1 , wherein the powders of the one or more alloying elements is selected because it will render the gun carrier degradable in fluid having a pH less than 7.0.
Aluminium-based alloys · CPC title
Both compacting and sintering (by forging B22F3/17) · CPC title
Sintering only · CPC title
After-treatment of workpieces or articles {(B22F3/1146 takes precedence)} · CPC title
by forging · CPC title