High-strength cold-rolled steel sheet having excellent surface quality and low material variation, and method for manufacturing same
US-2024384366-A1 · Nov 21, 2024 · US
US9767946B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9767946-B2 |
| Application number | US-201314418351-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 1, 2013 |
| Priority date | Aug 21, 2012 |
| Publication date | Sep 19, 2017 |
| Grant date | Sep 19, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A non-oriented electrical steel sheet has a chemical composition having C: not more than 0.005 mass %, Si: 2-7 mass %, Mn: 0.033 mass %, Al: not more than 3 mass %, P: not more than 0.2 mass %, S: not more than 0.005 mass %, N: not more than 0.005 mass %, Se: 0.0001˜0.0005 mass %, As: 0.0005˜0.005 mass % and the remainder being Fe and inevitable impurities, and an iron loss W 15/50 in excitation at 50 Hz and 1.5 T of not more than 3.5 W/kg and a ratio (x/t) of amount of shear drop x (mm) to thickness t (mm) in punching of steel sheet of not more than 0.15 and is excellent in the iron loss property before punching and less in the deterioration of the iron loss property by punching.
Opening claim text (preview).
The invention claimed is: 1. A non-oriented electrical steel sheet having chemical composition comprising C: not more than 0.005 mass %, Si: 2˜7 mass %, Mn: 0.03˜3 mass %, Al: not more than 3 mass %, P: not more than 0.2 mass %, S: not more than 0.005 mass %, N: not more than 0.005 mass %, Se: 0.0001˜0.0005 mass %, As: 0.0005˜0.005 mass % and the remainder being Fe and inevitable impurities, and an iron loss W 15/50 in excitation at 50 Hz and 1.5 T of not more than 3.5 W/kg, a ratio (x/t) of amount of shear drop x (mm) to thickness t (mm) in punching of steel sheet of not more than 0.15, and an average crystal grain size of 30˜150 μm. 2. The non-oriented electrical steel sheet according to claim 1 containing either one or both of Sn: 0.003˜0.5 mass % and Sb: 0.003˜0.5 mass % in addition to the chemical composition.
following hot rolling · CPC title
containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60 · CPC title
containing N · CPC title
containing aluminium · CPC title
containing tin · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.