Reciprocating-plate column reactor for epoxidation of epoxy resins
US-9527950-B2 · Dec 27, 2016 · US
US9765179B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9765179-B2 |
| Application number | US-201414890237-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 15, 2014 |
| Priority date | May 15, 2013 |
| Publication date | Sep 19, 2017 |
| Grant date | Sep 19, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed is a method for producing a biphenyl-skeleton-containing epoxy resin represented by Formula (1) described below including a step of allowing polyvalent hydroxy biphenyl obtained by a production step including a regioselective cross-coupling reaction to react with epihalohydrin. (In the formula, k1 and l1 each represent an integer of 0 to 4, m and n each represent an integer of 1 to 5, R 1 and R 2 each independently represent a hydrocarbon group having 1 to 10 carbon atoms which may have a substituent group, and R 1 and R 2 may be identical to each other or different from each other. (Provided that left and right phenyl structures of a biphenyl skeleton are different from each other.)
Opening claim text (preview).
The invention claimed is: 1. A method for producing a biphenyl-skeleton-containing epoxy resin represented by Formula (1) described below, comprising: a step of allowing a polyvalent hydroxy biphenyl obtained by a production step including a regioselective cross-coupling reaction to react with epihalohydrin: in the formula, k1 and l1 each represent an integer of 0 to 4, m and n each represent an integer of 1 to 5, R 1 and R 2 each independently represent a hydrocarbon group having 1 to 10 carbon atoms which may have a substituent group, and R 1 and R 2 may be identical to each other or different from each other, provided that left and right phenyl structures of a biphenyl skeleton are different from each other. 2. The method for producing a biphenyl-skeleton-containing epoxy resin according to claim 1 , wherein the regioselective cross-coupling reaction is a cross-coupling reaction between at least one compound selected from aryl boronic acids and an anhydride thereof, ester and a borate salt represented by Formula (2) described below, and at least one compound selected from aryl halide or aryl sulfonate represented by Formula (3) described below: k1 and l1 each represent an integer of 0 to 4, m and n each represent an integer of 1 to 5, R 1 and R 2 each independently represents a hydrocarbon group having 1 to 10 carbon atoms which may have a substituent group, R 1 and R 2 may be identical to each other or different from each other, R 3 and R 4 each independently represent a hydrogen atom, a methyl group, a benzyl group, a tetrahydropyranyl group, a tetrahydrofuryl group, a methoxymethyl group, an ethoxymethyl group, a silyl group, a trimethyl silyl group, a tert-butyl dimethyl silyl group, or a triisopropyl silyl group, and X represents a chlorine atom, a bromine atom, an iodine atom, triflate, mesylate, tosylate, or nosylate.
with epihalohydrins · CPC title
Polycondensates containing more than one epoxy group per molecule · CPC title
linked by a carbon chain containing aromatic rings · CPC title
Ethers of oxirane-containing polyhydroxy compounds in which all hydroxyl radicals are etherified with oxirane-containing hydroxy compounds · CPC title
containing three or more hetero rings · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.