Electrically conductive thin films
US-2015376020-A1 · Dec 31, 2015 · US
US9701542B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9701542-B2 |
| Application number | US-201414175697-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 7, 2014 |
| Priority date | Jan 16, 2013 |
| Publication date | Jul 11, 2017 |
| Grant date | Jul 11, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The presently disclosed and/or claimed inventive concept(s) relates generally to hexagonal osmium boride, OsB 2 , and methods of producing the same. In one non-limiting embodiment, hexagonal OsB 2 is produced by mechanochemical synthesis of osmium and boron in a high energy ball mill.
Opening claim text (preview).
What is claimed is: 1. A method of producing a bulk form of OsB 2 wherein the OsB 2 has a hexagonal lattice structure, comprising the steps of (i) mechanochemically reacting osmium and boron for at least 6 hours to form a hexagonal OsB 2 powder and (ii) sintering the hexagonal OsB 2 powder to form a sintered bulk form of OsB 2 . 2. The method of claim 1 , wherein the osmium and boron are mechanochemically reacted in a high energy ball mill. 3. The method of claim 1 , wherein the osmium and boron are in the form of powders. 4. The method of claim 3 , wherein the osmium powder and boron powder are added at a molar ratio in a range of from about 1:2 to about 1:3 osmium powder to boron powder. 5. The method of claim 1 , wherein the osmium and boron powders are mechanochemically reacted for at least 20 hours. 6. The method of claim 1 , wherein the hexagonal OsB 2 powder is sintered by high temperature Spark Plasma Sintering at a temperature of at least about 1550° C. and at a pressure of at least about 50 MPa. 7. The method of claim 1 , wherein the osmium and boron powders are mechanochemically reacted for at least 18 hours.
Inorganic compounds or compositions · CPC title
by solid state reactions or multi-phase diffusion · CPC title
Metal borides · CPC title
submicron sized, i.e. from 0,1 to 1 micron · CPC title
Phases present in the sintered or melt-cast ceramic products other than the main phase · CPC title