A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A polyester prepared by free radical polymerization of an unsaturated polyester prepolymer, wherein the polymerization occurs primarily by reaction of the unsaturation of said prepolymer is disclosed. Coatings comprising the same are also disclosed, as are substrates coated at least in part with such coating.
Opening claim text (preview).
The invention claimed is: 1. A coating composition comprising a polyester resin and a crosslinker therefor; the polyester resin being an ungelled crosslinkable polyester resin comprising: (a) reacting a polycarboxylic acid with a polyol to form an unsaturated polyester prepolymer in which the unsaturation is along the backbone of the unsaturated polyester prepolymer and wherein the unsaturated polyester prepolymer has terminal acid and/or hydroxyl functional groups, (b) subjecting the unsaturated polyester prepolymer to free radical polymerization via the points of unsaturation along the unsaturated polyester prepolymer backbone to form the ungelled crosslinkable polyester resin that has a weight average molecular weight of 10,000 to 4,000,000 and that has a higher weight average molecular weight than the unsaturated polyester prepolymer such that the weight average molecular weight ratio of the ungelled crosslinkable polyester resin to the unsaturated polyester prepolymer is at least 1.2 and the hydroxyl value and the acid value of the ungelled crosslinkable polyester resin is in the same range as those of the prepolymer; wherein the hydroxyl value of the unsaturated polyester prepolymer ranges from 2 to 500 mg KOH/gm and/or the acid value of the unsaturated polyester prepolymer ranges from 1 to 400 mg KOH/gm. 2. The coating composition of claim 1 in which the crosslinker comprises a phenolic resin or an aminoplast. 3. A package coated with the coating composition of claim 1 . 4. The package of claim 3 wherein the package is a metal can.
Elemental metal containing [e.g., substrate, foil, film, coating, etc.] · CPC title
Next to polyester, polyamide or polyimide [e.g., alkyd, glue, or nylon, etc.] · CPC title
containing two or more polymers of the same C08L -group · CPC title
Peroxy-compounds · CPC title
Polycarboxylic acids or polyhydroxy compounds in which at least one of the two components contains aliphatic unsaturation · CPC title