A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Polyurethane floor covering products are formed from a web layer containing at least 30% by weight fibers. A cooled polyurethane foam formulation which includes at least one polyisocyanate, water and at least one polyol having an equivalent weight of at least 500 is applied to the web layer. The wetted web layer is then compressed to mechanically wet out the fibers, gauged and heated to cure the foam formulation.
Opening claim text (preview).
What is claimed is: 1. A process for preparing a foamed polyurethane floor covering product that includes a cured and gauged polyurethane foam cushion containing from 5 to 50% by weight of the fibers, comprising: a) forming a web layer containing at least 30% by weight fibers, such that the web layer has a weight of from 150 to 660 g/m 2 and a thickness of 0.25 to 1 inch, and the fibers in the web layer have an average length of from 7 to 140 cm and a denier of 5 to 50; b) continuously applying a cooled polyurethane foam formulation which includes at least one polyisocyanate, water and at least one polyol having an equivalent weight of at least 500 to the web layer, the cooled polyurethane foam formulation having a temperature of no more than 15° C. when applied to the web layer, and compressing the web layer and applied polyurethane foam formulation together to 5 to 35% of the original thickness of the web layer to mechanically wet out the fibers in the web layer; and then c) gauging the wetted web layer to a thickness of from 0.25 to 1.0 inches and, while maintaining the gauge, heating the polyurethane foam formulation to a temperature of from 80 to 160° C. to cure the polyurethane foam formulation to produce a cured and gauged polyurethane foam cushion containing from 5 to 30% by weight of the fibers. 2. The process of claim 1 , wherein the cooled polyurethane foam formulation has a temperature of not more than 10° C. when applied to the web layer. 3. The process of claim 1 , wherein the web layer contains at least 50% by weight of fibers. 4. The process of claim 1 , wherein the web layer comprises carded fibers. 5. The process of claim 1 , wherein the fibers are obtained from postconsumer carpeting products. 6. The process of claim 1 , wherein the foamed polyurethane floor covering product has a density of from 3 to 10 pounds/cubic foot (48-160 kg/m 3 ). 7. A foamed polyurethane floor covering product produced by the process of claim 1 .
Scraps or recycled materials (D06N2205/106 takes precedence) · CPC title
Foam · CPC title
with polyurethanes · CPC title
the preformed parts being three-dimensional structures · CPC title
Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof}, as moulding material · CPC title