Methods and systems of joining pipes

US9683682B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9683682-B2
Application numberUS-201313833552-A
CountryUS
Kind codeB2
Filing dateMar 15, 2013
Priority dateAug 3, 2012
Publication dateJun 20, 2017
Grant dateJun 20, 2017

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A system and method is provided for joining pipes where a keyhole is formed in each of the pipe ends and then a filler metal is placed in the keyholes to join the pipes to each other. The filler metal can be deposited using a laser hot wire process.

First claim

Opening claim text (preview).

The invention claimed is: 1. A method of forming a joint between a first pipe of a first base material and a second pipe of a second base material, the method comprising: disposing the second pipe coaxially within the first pipe to define a pipe joint axis; forming at least one keyhole extending at least partially through the first and second pipes with a beam from a first heat source; forming a weld metal in the at least one keyhole from a filler wire connected to a power supply; rotating the first and second pipes relative the filler wire and the first heat source; and forming an arc with the wire in the keyhole. 2. The method of claim 1 , wherein forming the at least one keyhole includes delivering a laser beam to the first and second pipes. 3. The method of claim 2 , wherein delivering the laser beam includes delivering the laser beam with a first energy density to the first pipe and delivering the laser beam to the second pipe with a second energy density, the second energy density being different from the first energy density. 4. The method of claim 2 , wherein delivering the laser beam includes delivering the laser beam with a first energy density to the first pipe and delivering the laser beam to the second pipe with a second energy density, the second energy density being the same as the first energy density. 5. The method of claim 2 , wherein delivering the laser beam includes delivering the laser beam with an enemy density being a function of the first and second materials. 6. The method of claim 2 , wherein forming the weld metal includes controlling the depth in which a molten puddle is maintained within the keyhole, the depth being controlled by controlling the energy density of the laser beam to the keyhole. 7. The method of claim 1 , wherein forming the weld metal include tapering the weld metal within the keyhole. 8. The method of claim 1 , wherein forming the at least one keyhole forms the keyhole completely through the first and second pipe materials toward the joint axis. 9. The method of claim 1 , further comprising disposing a sleeve between the first and the second pipe. 10. The method of claim 1 , wherein forming the at least one keyhole includes axially spacing a plurality of keyholes spaced apart along the pipe joint axis. 11. A method of forming a joint between a first pipe of a first base material and a second pipe of a second base material, the method comprising: disposing the second pipe coaxially with respect to the first pipe to define a pipe joint axis; disposing a sleeve between the first and second pipe so as to interconnect the first and second pipes; forming at least one keyhole extending at least partially through a least one of the first pipe and the second pipe and through the sleeve with a beam from a first heat source; forming a weld metal in the at least one keyhole from a filler wire connected to a power supply; rotating the first pipe, second pipe and sleeve relative the filler wire and the first heat source; and forming an arc with the wire in the keyhole. 12. The method of claim 11 , wherein disposing the second pipe includes disposing the second pipe within the first pipe, and disposing the sleeve including disposing the sleeve within the first pipe and outside the second pipe. 13. The method of claim 11 , wherein disposing the second pipe includes disposing the second pipe so as not to overlap the first pipe, and disposing the sleeve within the first pipe and the second pipe. 14. The method of claim 11 , wherein disposing the second pipe includes disposing the second pipe so as not to overlap the first pipe, and disposing the sleeve outside the first pipe and the second pipe. 15. The method of claim 11 , further comprising disposing a weld bead between the sleeve and the first and second pipes. 16. The method of claim 11 , wherein forming the at least one keyhole includes axially spacing a plurality of keyholes spaced apart along the pipe joint axis. 17. The method of claim 11 , wherein forming the at least one keyhole includes delivering a laser beam to the first and second pipes. 18. The method of claim 17 , wherein delivering the laser beam includes delivering the laser beam with a first energy density to the first pipe and delivering the laser beam to the second pipe with a second energy density, the second energy density being different from the first energy density. 19. The method of claim 11 , wherein delivering the laser beam includes delivering the laser beam with a first energy density to the first pipe and delivering the laser beam to the second pipe with a second energy density the second energy density being the same as the first energy density. 20. The method of claim 11 , wherein delivering the laser beam includes delivering the laser beam with an energy density being a function of the first and second materials. 21. The method of claim 11 , wherein forming the weld metal includes controlling the depth in which a molten puddle is maintained within the keyhole, a depth being controlled by controlling the energy density of the laser beam to the keyhole. 22. The method of claim 11 , wherein forming the weld metal include tapering the weld metal within the keyhole. 23. A method of forming a joint between a first pipe of a first base material and a second pipe of a second base material, the method comprising: disposing the second pipe coaxially with respect to the first pipe to define a pipe joint axis; disposing a sleeve between the first and second pipe so as to interconnect the first and second pipes; forming at least one keyhole extending at least partially through at least one of the first pipe and the second pipe and through the sleeve with a beam from a first heat source; forming a weld metal in the at least one keyhole from a filler wire heated by a second heat source; and rotating the first pipe, second pipe and sleeve relative to the filler wire and the first heat source, wherein forming the weld metal includes delivering the filler wire to the at least one keyhole so as to maintain the filler wire in continuous contact with a molten puddle in the keyhole.

Assignees

Inventors

Classifications

  • Ferrous alloys and aluminium or alloys thereof · CPC title

  • Dissimilar materials · CPC title

  • Tubes · CPC title

  • with holes in the sleeve or spigot being filled with weld · CPC title

  • of tube sections · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9683682B2 cover?
A system and method is provided for joining pipes where a keyhole is formed in each of the pipe ends and then a filler metal is placed in the keyholes to join the pipes to each other. The filler metal can be deposited using a laser hot wire process.
Who is the assignee on this patent?
Lincoln Global Inc
What technology area does this patent fall under?
Primary CPC classification F16L13/0245. Mapped technology areas include Mechanical Engineering.
When was this patent published?
Publication date Tue Jun 20 2017 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).