Separator for nonaqueous cell and nonaqueous cell
US-2015079479-A1 · Mar 19, 2015 · US
US9653717B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9653717-B2 |
| Application number | US-201414468642-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 26, 2014 |
| Priority date | Aug 30, 2013 |
| Publication date | May 16, 2017 |
| Grant date | May 16, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A separator for electrochemical element, comprising a porous sheet that contains as a main fiber, a fibrillated solvent spun cellulose fiber with an average fiber length of 0.40 to 1.10 mm, has an average internal bond strength of 60 mJ or more in a thickness direction, and has a lowest internal bond strength of 30 mJ or more in the thickness direction, a process for producing the separator, and an electrochemical element using the separator. The separator for electrochemical element has strong mechanical strength and excellent processability.
Opening claim text (preview).
What is claimed is: 1. A separator for electrochemical element, comprising a porous sheet that contains as a main fiber, a fibrillated solvent spun cellulose fiber with an average fiber length of 0.40 to 1.10 mm, has an average internal bond strength of 60 mJ or more in a thickness direction, and has a lowest internal bond strength of 30 mJ or more in the thickness direction. 2. A process for producing a separator for electrochemical element, comprising a porous sheet that contains as a main fiber, a fibrillated solvent spun cellulose fiber with an average fiber length of 0.40 to 1.10 mm, has an average internal bond strength of 60 mJ or more in a thickness direction, and has a lowest internal bond strength of 30 mJ or more in the thickness direction, wherein the porous sheet is prepared by a paper-making method, in which a wet press treatment of two or more nips is performed at least on the porous sheet. 3. A process for producing a separator for electrochemical element, comprising a porous sheet that contains as a main fiber, a fibrillated solvent spun cellulose fiber with an average fiber length of 0.40 to 1.10 mm, has an average internal bond strength of 60 mJ or more in a thickness direction, and has a lowest internal bond strength of 30 mJ or more in the thickness direction, wherein the porous sheet is prepared by a paper-making method, in which both surfaces of the porous sheet are contacted with a heated cylinder roll at least once. 4. A separator for electrochemical element produced by the process for producing the separator for electrochemical element recited in claim 2 . 5. An electrochemical element comprising the separator for electrochemical element recited in claim 1 . 6. A separator for electrochemical element produced by the process for producing the separator for electrochemical element recited in claim 3 . 7. An electrochemical element comprising the separator for electrochemical element recited in claim 4 . 8. An electrochemical element comprising the separator for electrochemical element recited in claim 6 .
Moulding; Embossing; Cutting · CPC title
Highly hydrated, swollen or fibrillatable fibres · CPC title
Synthetic cellulose fibres · CPC title
Electricity · mapped topic
Electricity · mapped topic
Related publications grouped by family.
Answers are generated from the same data shown on this page.