Process for the manufacture of paper and paperboard
US-2015345081-A1 · Dec 3, 2015 · US
US9598819B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9598819-B2 |
| Application number | US-201414535692-A |
| Country | US |
| Kind code | B2 |
| Filing date | Nov 7, 2014 |
| Priority date | Nov 8, 2013 |
| Publication date | Mar 21, 2017 |
| Grant date | Mar 21, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of treating a cellulosic slurry to improve drainage is disclosed; the method comprises adding a surfactant based brown stock wash aid to a cellulosic furnish in an amount of from 0.5 to 1 lbs per ton and adding a synthetic polymer papermachine drainage or strength aid to the furnish in an amount of from 0.1 to 10 lbs per ton, allowing the furnish to drain and forming a paper product.
Opening claim text (preview).
The invention claimed is: 1. A method of treating an unbleached cellulosic furnish to improve drainage comprising adding a surfactant based brown stock wash aid comprising 5 to 30% of a triblock copolymer of polyethylene glycol and poly propylene glycol, 5 to 40% of an alcohol ethoxylate, and 2 to 20% of a copolymer of polyisobutylene and sodium polymaleate to the cellulosic furnish in an amount of from 0.01 to 10 lbs per ton of furnish solids and adding a cationic polyacrylamide papermachine drainage or strength aid to the cellulosic furnish in an amount of from 0.01 to 10 lbs per ton of furnish solids, allowing the cellulosic furnish to drain and forming an unbleached paper product. 2. The method of claim 1 wherein the synthetic polymer papermachine drainage or strength aid has a viscosity average molecular weight of 1,000,000 to 25,000,000 Daltons. 3. The method of claim 1 wherein the synthetic polymer papermachine drainage or strength aid has a viscosity average molecular weight of 500,000 to 5,000,000 Daltons. 4. The method of claim 1 wherein the cationic polymer is made using at least one cationic monomer selected from the group consisting of diallyldialkylammonium halides; the (meth)acrylates of dialkylaminoalkyl compounds and the salts and quaternaries thereof; the N,N-dialkylaminoalkyl(meth)acrylamides and the salt and quaternaries thereof and mixtures of the foregoing. 5. The method of claim 1 wherein the weight ratio of the surfactant based brown stock wash aid to synthetic polymer papermachine drainage or strength aid is in the range of from 80:20 to 20:80. 6. The method of claim 1 wherein amount of synthetic polymer papermachine drainage or strength aid added to the furnish is from 0.05 to 5 lbs of synthetic polymer per ton of furnish solids. 7. The method of claim 1 wherein the cellulosic furnish has a soluble lignin level of from 25 ppm up to 2500 ppm. 8. The method of claim 1 wherein amount of surfactant based brown stock wash aid added is from 0.1 to 2 lbs solids per ton of furnish solids. 9. The method of claim 1 wherein the cationic polymer is made using at least one cationic monomer selected from the group consisting of diallyldimethylammonium chloride; dimethylaminoethyl (meth)acrylate, diethylaminoethyl (meth)acrylate, dimethyl aminopropyl (meth)acrylate, 2-hydroxydimethyl aminopropyl (meth)acrylate, aminoethyl (meth)acrylate, and the salts and quaternaries thereof; N,N-dimethylaminoethyl acrylamide, and the salt and quaternaries thereof and mixtures of the foregoing. 10. The method of claim 1 wherein amount of surfactant based brown stock wash aid added is from 0.05 to 5 lbs solids per ton of furnish solids. 11. A method of treating an unbleached cellulosic furnish comprising adding a surfactant based brown stock wash aid to an unbleached cellulosic furnish in an amount of from 0.1 to 10 lbs per ton and adding a synthetic polymer papermachine drainage or strength aid to the furnish in an amount of from 0.1 to 10 lbs per ton furnish solid allowing the furnish to drain and forming an unbleached paper product, wherein the brown stock wash comprises at least one anionic surfactant and at least one nonionic surfactant, and di-block and tri-block copolymers of polyethylene glycol and polypropylene glycol, wherein the anionic surfactant is selected from the group consisting of alkylbenzene sulfonates, dialkyl sulfosuccinates, alkyl sulfonates, alkyl phosphates, alkyl carboxylates, where the alkyl chain can be linear or branched; “poly(meth)acrylates; polymaleic acid and anhydrides; and lignosulfonates; and wherein the at least one non ionic surfactant is selected from the group consisting of nonyl phenol ethoxylates; linear and branched alcohol alkoxylates; sorbitan esters; alkoxylated sorbitan alkyl esters; and wherein the weight ratio of the nonionic surfactant to the anionic surfactant is from 5:95 to 95:5. 12. A method of treating an unbleached cellulosic furnish comprising adding a surfactant based brown stock wash aid to an unbleached cellulosic furnish in an amount of from 0.1 to 10 lbs per ton and adding a synthetic polymer papermachine drainage or strength aid to the furnish in an amount of from 0.1 to 10 lbs per ton furnish solid allowing the furnish to drain and forming an unbleached paper product, wherein the brown stock wash comprises at least one anionic surfactant, at least one nonionic surfactant, and at least one surfactant formed from a polymaleic acid and an anhydride, wherein the anionic surfactant is selected from the group consisting of alkylbenzene sulfonates, dialkyl sulfosuccinates, alkyl sulfonates, alkyl phosphates, alkyl carboxylates, where the alkyl chain can be linear or branched; “poly(meth)acrylates; and lignosulfonates; and wherein the at least one non ionic surfactant is selected from the group consisting of nonyl phenol ethoxylates; linear and branched alcohol alkoxylates; sorbitan esters; alkoxylated sorbitan alkyl esters; di-block or tri-block copolymers of polyethylene glycol and polypropylene glycol; and wherein the weight ratio of the nonionic surfactant to the anionic surfactant is from 1:99 to 99:1.