Expandable vinyl aromatic polymers comprising platelet needle coke particles
US-2015353701-A1 · Dec 10, 2015 · US
US9593236B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9593236-B2 |
| Application number | US-201414583986-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 29, 2014 |
| Priority date | Dec 31, 2013 |
| Publication date | Mar 14, 2017 |
| Grant date | Mar 14, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided are a preparation method of a thermoplastic resin composition and a thermoplastic resin composition prepared therefrom. The preparation method includes: feeding a first thermoplastic resin in a molten state into a first hopper and feeding an impact reinforcing agent including a predetermined content of moisture into a second hopper, followed by kneading and extruding processes, and removing the moisture in a first vent port and a second vent port, wherein the first hopper, the first vent port, the second hopper, a first kneading zone, and the second vent port are sequentially formed in a moving direction of an extruder. The thermoplastic resin composition prepared therefrom can have improved appearance property and improved color property by removing moisture of an impact reinforcing agent added to the thermoplastic resin composition.
Opening claim text (preview).
What is claimed is: 1. A preparation method of a thermoplastic resin composition comprising: feeding a first thermoplastic resin in a molten state into a first hopper and feeding an impact reinforcing agent including a predetermined content of moisture into a second hopper, followed by kneading and extruding processes, and removing the moisture in a first vent port and a second vent port, wherein the first hopper, the first vent port, the second hopper, a first kneading zone, and the second vent port are sequentially formed in a moving direction of an extruder. 2. The preparation method of claim 1 , wherein the first vent port is an opened vent without a separate apparatus, and the second vent port is provided with an apparatus selectively extracting steam only. 3. The preparation method of claim 1 , wherein a moisture content W 1 removed in the first vent port and a moisture content W 2 removed in the second vent port have a weight ratio (W 1 /W 2 ) of about 0.5 to about 25. 4. The preparation method of claim 1 , wherein a moisture content removed in the first vent port corresponds to about 60 to about 90 wt % of the total moisture content of the first thermoplastic resin and the impact reinforcing agent, and a moisture content removed in the second vent port corresponds to about 10 to about 40 wt % of the total moisture content of the first thermoplastic resin and the impact reinforcing agent. 5. The preparation method of claim 1 , wherein the first thermoplastic resin is an aromatic vinyl-vinyl cyanide-based copolymer, and the impact reinforcing agent is a rubber-modified vinyl-based graft copolymer. 6. The preparation method of claim 5 , wherein the first thermoplastic resin is at least one selected from the group consisting of a styrene-acrylonitrile copolymer, an α-methyl styrene-acrylonitrile copolymer, and a styrene-a-methyl styrene-acrylonitrile copolymer, and the impact reinforcing agent is an acrylonitrile-butadiene-styrene graft copolymer (g-ABS) obtained by graft copolymerization with about 30 to about 70 wt % of a mixture containing an aromatic vinyl-based compound and a vinyl cyanide-based compound in the presence of about 30 to about 70 wt % of a rubber-like polymer, using emulsion polymerization. 7. The preparation method of claim 1 , wherein a second kneading zone and a third vent port are further formed after the second vent port. 8. The preparation method of claim 7 , wherein the third vent port includes a vacuum vent, and removes at least one selected from the group consisting of residual water, unreacted monomers, oligomers, and decomposition gases.
Aromatic polyamides [polyaramides] or derivatives thereof · CPC title
through a degassing opening of a barrel · CPC title
at several locations, e.g. using several hoppers or using a separate additive feeding · CPC title
characterised by the choice of material · CPC title
Removing undesirable residual components, e.g. solvents, unreacted monomers; Degassing · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.