Hydrophilic block copolymers and membranes prepared therefrom (i)
US-2015376340-A1 · Dec 31, 2015 · US
US9587112B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9587112-B2 |
| Application number | US-201013498877-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 14, 2010 |
| Priority date | Sep 29, 2009 |
| Publication date | Mar 7, 2017 |
| Grant date | Mar 7, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
According to the present invention, an aromatic polysulfone resin is offered which is suitable as film material, especially in porous membranes. The aromatic polysulfone resin of the present invention has a reduced viscosity of 0.55-0.65 dL/g, and preferably 0.58-0.62 dL/g, number average molecular weight (Mn) of 22000 or more, and preferably 23500 or more, and a value of the ratio of weight average molecular weight (Mw) relative to number average molecular weight (Mn) of 2.54 or less, and preferably 2.50 or less.
Opening claim text (preview).
The invention claimed is: 1. Aromatic polysulfone resin, wherein reduced viscosity is 0.55-0.65 dL/g, number average molecular weight (Mn) is 22000 or more, a value of the ratio (Mw/Mn) of weight average molecular weight (Mw) relative to number average molecular weight (Mn) is 2.54 or less, and a proportion of a repeating unit represented by a formula (1) is 80 to 100 mol %, relative to the total of all repeating units, Ph 1 -SO 2 -Ph 2 -O— (1) wherein Ph 1 and Ph 2 each independently represent a phenylene group, and hydrogen atoms of the aforementioned phenylene groups may each be independently substituted with one of an alkyl group, an aryl group, and a halogen atom. 2. Film comprising the aromatic polysulfone resin according to claim 1 . 3. The film according to claim 2 , which is a porous membrane. 4. The aromatic polysulfone resin according to claim 1 , wherein the reduced viscosity is 0.58-0.62 dL/g. 5. The aromatic polysulfone resin according to claim 1 , wherein the number average molecular weight (Mn) is 23500 to 27000. 6. The aromatic polysulfone resin according to claim 4 , wherein the number average molecular weight (Mn) is 23500 to 27000. 7. Film comprising the aromatic polysulfone resin according to claim 4 . 8. Film comprising the aromatic polysulfone resin according to claim 5 . 9. Film comprising the aromatic polysulfone resin according to claim 6 . 10. The film according to claim 7 , which is a porous membrane. 11. The film according to claim 8 , which is a porous membrane. 12. The film according to claim 9 , which is a porous membrane.
Drying · CPC title
Polysulfones; Polyethersulfones · CPC title
Specific permeability or cut-off range · CPC title
characterised by their properties · CPC title
Polysulfones; Polyethersulfones · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.