Sealing propylene copolymer
US-9243137-B2 · Jan 26, 2016 · US
US9567418B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9567418-B2 |
| Application number | US-201415032694-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 24, 2014 |
| Priority date | Oct 30, 2013 |
| Publication date | Feb 14, 2017 |
| Grant date | Feb 14, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present disclosure relates to a propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt % to 3.0 wt %; ii) a melt flow rate (MFR) measured according to the method ISO 1133 (230° C., 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min; iii) a polydispersity (PI) ranges from 4.5 to 10 and the distribution of molecular weight is of multimodal type; iv) a melting point ranging from 160° C. to 145° C.; and v) a differential scanning calorimetry (DSC) curve (temperature/heat of fusion) that shows at least two peaks.
Opening claim text (preview).
What is claimed is: 1. A propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt % to 3.0 wt %; ii) a melt flow rate (MFR) measured according to the method ISO 1133 (230° C., 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min; iii) a polydispersity index (PI) ranging from 4.5 to 10 where the distribution of molecular weight is of a multimodal type; iv) a melting point ranging from 145−160° C.; and v) a differential scanning calorimetry (DSC) curve (temperature/heat of fusion) that shows at least two peaks. 2. The propylene-hexene-1 copolymer according to claim 1 , wherein the content of 1-hexene derived units ranges from 0.7 wt % to 2.0 wt %. 3. The propylene-hexene-1 copolymer according to claim 1 , wherein the melt flow rate (MFR) measured according to the method ISO 1133 (230° C., 5 kg) ranges from 0.6 g/10 min to 4.0 g/10 min. 4. The propylene-hexene-1 copolymer according claim 1 , wherein the melting point ranges from 147-155° C. 5. An industrial sheet comprising the propylene-1-hexene copolymer of claim 1 .
Manufacture of films or sheets · CPC title
Copolymers of propene (C08J2323/16 takes precedence) · CPC title
Propene · CPC title
Copolymers of propene (C08L23/16 takes precedence) · CPC title