Method for manufacturing quantum dot light-emitting element and display device using quantum dot
US-2016293875-A1 · Oct 6, 2016 · US
US9559322B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9559322-B2 |
| Application number | US-201414244874-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 3, 2014 |
| Priority date | Apr 5, 2013 |
| Publication date | Jan 31, 2017 |
| Grant date | Jan 31, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
In a method of manufacturing a quantum dot, a core may be formed using (utilizing) at least one cation precursor and at least one anion precursor. The core may be reacted with a shell forming precursor and a ligand forming precursor for more than one hour to form a shell enclosing the core and a ligand. A nanoparticle including the core, the shell and the ligand may be washed.
Opening claim text (preview).
What is claimed is: 1. A method of manufacturing a quantum dot, the method comprising: forming a core utilizing at least one cation precursor and at least one anion precursor; reacting the core with a mixture comprising a shell forming anion precursor solution without an additional cation precursor for more than one hour to form a first shell surrounding the core, the anion of the shell forming anion precursor being one or more elements in Group XVI; washing a nanoparticle comprising the core and the first shell; reacting a second shell forming precursor with the core and the first shell to form a second shell enclosing the first shell; and reacting a ligand forming precursor with the core and the first and second shells to form a ligand on a surface of the second shell, the ligand forming precursor being oleic acid or a mixture of oleic acid and trialkylphosphine. 2. The method of claim 1 , wherein the forming of the core comprises: forming a mixture comprising the at least one cation precursor, an organic solvent and an unsaturated fatty acid, the cation precursor being selected from the group consisting of an element in Group XII and an element in Group XIII; heating the mixture; and adding the at least one anion precursor to the mixture to react the anion precursor and the cation precursor, the anion precursor being selected from the group consisting of an element in Group XV and an element in Group XVI. 3. The method of claim 1 , wherein the cation precursor comprises zinc (Zn), cadmium (Cd) and/or indium (In), and the anion precursor comprises sulfur (S), selenium (Se), tellurium (Te) and/or phosphorous (P). 4. The method of claim 1 , wherein the ligand forming precursor is oleic acid. 5. The method of claim 1 , wherein the second shell forming precursor comprises at least one element in Group XII and at least one element in Group XVI. 6. The method of claim 1 , wherein the washing of the nanoparticle comprises: precipitating the nanoparticle in a non-polar solvent; and centrifuging the nanoparticle. 7. A method of manufacturing an organic light emitting display device, the method comprising: forming an anode on a substrate; forming a hole injection layer (HIL) on the anode; forming a hole transport layer (HTL) on the HIL; forming an emitting layer (EML) on the HTL utilizing a quantum dot having a size above about 10 nm, the quantum dot comprising a core, a first shell and a second shell enclosing the core, and a ligand on a surface of the second shell, the ligand being oleate or a mixture of oleate and trioctylphosphine; forming an electron transport layer (ETL) on the EML; and forming a cathode directly on the ETL, wherein the forming of the emitting layer comprises reacting the core with a mixture comprising a shell forming anion precursor solution without an additional cation precursor for more than one hour to form the first shell surrounding the core, the anion of the shell forming anion precursor being one or more elements in Group XVI. 8. The method of claim 7 , wherein the HTL comprises polyvinylcarbazole. 9. The method of claim 7 , wherein the forming of the EML on the HTL comprises dispersing the quantum dot on the HTL utilizing a solvent comprising hexane.
Electricity · mapped topic
with zinc or cadmium · CPC title
Electricity · mapped topic
non-luminescent particle coatings or suspension media · CPC title
with zinc cadmium · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.