Bottle and method of using
US-2019337686-A1 · Nov 7, 2019 · US
US9555948B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9555948-B2 |
| Application number | US-201314100594-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 9, 2013 |
| Priority date | Dec 9, 2013 |
| Publication date | Jan 31, 2017 |
| Grant date | Jan 31, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A double-walled, vacuum-insulated container is manufactured with a cured inside coating. To form the container, an inner liner is disposed in an outer body. The inner liner has an inner sidewall, an inner bottom, and an inner lip, and the outer body has an outer sidewall and an outer lip. The inner and outer lips are affixed together with an affixation or weld having a first melt point. A plenum is enclosed between the inner liner and the outer body by affixing an outer bottom to the outer body and creating a vacuum at least partially in the plenum using a seal having a second melt point. This second melt point can be about 450° C. and 500° C. The coating is painted to an inside surface of the inner liner, and the painted coating is cured with a temperature level at least below the first and second melt points.
Opening claim text (preview).
What is claimed is: 1. A container manufacturing method, comprising: forming a double-walled container having a plenum enclosed between an inner body and an outer body; creating a vacuum at least partially in the plenum using a seal having a first melt point; applying a paint coating to an inside surface of the inner body after creating the vacuum, the paint coating having a drying temperature above a normal drying temperature of a conventional paint coating; and curing the paint coating with a temperature level, the temperature level being above the normal drying temperature of the conventional paint coating and being below the first melt point. 2. The method of claim 1 , wherein the inner body and the outer body comprise a stainless steel material. 3. The method of claim 1 , wherein forming the double-walled container having the plenum enclosed between the inner body and the outer body comprises: disposing the inner body in the outer body, the inner body having an inner sidewall, an inner bottom, and an inner lip, the outer body having an outer sidewall and an outer lip; affixing the inner and outer lips together with an affixation having a second melt point; and enclosing the plenum between the inner body and the outer body by affixing an outer bottom to the outer body. 4. The method of claim 3 , comprising initially forming the inner body by affixing the inner bottom to an end of the inner sidewall. 5. The method of claim 4 , wherein affixing the inner bottom to the end of the inner sidewall comprises welding the inner bottom to the inner sidewall. 6. The method of claim 3 , wherein affixing the inner and outer lips together with the affixation having the second melt point comprises welding the inner and outer lips together. 7. The method of claim 3 , wherein affixing the outer bottom to the outer body comprises welding the outer bottom to the outer body. 8. The method of claim 3 , wherein curing the paint coating comprises curing the paint coating with the temperature level at least below the second melt point, wherein the second melt point is at least 500° C. 9. The method of claim 1 , wherein creating the vacuum in the plenum using the seal having the first melt point comprises drawing the vacuum from the plenum and sealing an evacuation port with the seal. 10. The method of claim 1 , wherein the first melt point is between 450° C. and 500° C. and the temperature level is 300° C. to 320° C. 11. The method of claim 1 , wherein curing the paint coating with the temperature level comprises passing the container through a heat tunnel at the temperature level approximately twice the normal drying temperature for the conventional paint coating, wherein the normal drying temperature for the conventional paint coating is about 160° C. 12. The method of claim 1 , wherein applying the paint coating to the inside surface of the inner liner comprises spraying the paint coating as a water-based ceramic paint onto the inside surface. 13. A double-walled, vacuum-insulated container manufactured according to the method of claim 1 . 14. A container manufacturing method, comprising: disposing an inner body in an outer body; affixing inner and outer lips of the inner and outer bodies together with an affixation having a first melt point; enclosing a plenum between the inner body and the outer body; creating a vacuum at least partially in the plenum using a seal having a second melt point; applying a paint coating to an inside surface of the inner body after creating the vacuum, the paint coating having a drying temperature above a normal drying temperature of a conventional paint coating; and curing the paint coating with a temperature level, the temperature level being above the normal drying temperature of the conventional paint coating and being below the first and second melt points. 15. The method of claim 14 , wherein curing the paint coating comprises curing the paint coating with the temperature level at least below the first melt point, wherein the first melt point is at least 500° C. 16. The method of claim 14 , wherein the second melt point is between 450° C. and 500° C. and the temperature level is 300° C. to 320° C. 17. The method of claim 14 , wherein curing the paint coating with the temperature level comprises passing the container through a heat tunnel at the temperature level approximately twice the normal drying temperature for the conventional paint coating, wherein the normal drying temperature for the conventional paint coating is about 160° C. 18. The method of claim 14 , wherein applying the paint coating to the inside surface of the inner liner comprises spraying the paint coating as a water-based ceramic paint onto the inside surface.
formed with double walls, i.e. hollow · CPC title
made of metal · CPC title
relating to soldering or welding · CPC title
Subsequently coating · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.