Conductive circuit containing a polymer composition containing thermally exfoliated graphite oxide and method of making the same
US-2015173188-A1 · Jun 18, 2015 · US
US9546092B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9546092-B2 |
| Application number | US-86630609-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 3, 2009 |
| Priority date | Feb 5, 2008 |
| Publication date | Jan 17, 2017 |
| Grant date | Jan 17, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Functionalized graphene sheets having a carbon to oxygen molar ratio of at least about 23:1 and method of preparing the same.
Opening claim text (preview).
The invention claimed is: 1. Functionalized graphene sheets having a carbon to oxygen molar ratio of at least about 23:1 and comprising fully exfoliated single sheets of graphene, and wherein the functionalized graphene sheets are dry. 2. The functionalized graphene sheets of claim 1 , wherein the carbon to oxygen ratio is at least about 28:1. 3. The functionalized graphene sheets of claim 1 , wherein the carbon to oxygen ratio is at least about 50:1. 4. The functionalized graphene sheets of claim 1 , wherein the carbon to oxygen ratio is at least about 75:1. 5. The functionalized graphene sheets of claim 1 further comprising functionalized graphene sheets having a surface area of between about 350 and about 2400 m 2 /g. 6. The functionalized graphene sheets of claim further comprising functionalized graphene sheets having a surface area of between about 400 and about 2400 m 2 /g. 7. The functionalized graphene sheets of claim 1 further comprising functionalized graphene sheets having a surface area of between about 500 and about 2400 m 2 /g. 8. The functionalized graphene sheets of claim 1 further comprising functionalized graphene sheets having a surface area of between about 800 and about 2400 m 2 /g. 9. A method for making functionalized graphene sheets as claimed in claim 1 , comprising heating graphite oxide and/or functionalized graphene sheets having a carbon to oxygen ratio of less than about 23:1 at a temperature of at least about 750° C. for a time sufficient to generate functionalized graphene sheets having a carbon to oxygen molar ratio of at least about 23:1 wherein the functionalized graphene sheets comprise fully exfoliated single sheets of graphene and wherein the functionalized graphene sheets are dry. 10. The method of claim 9 , wherein the temperature is at least about 850° C. and the heating time is at least about 2 minutes. 11. The method of claim 9 , wherein the temperature is at least about 950° C. and the heating time is at least about 2 minutes. 12. The method of claim 9 , wherein the heating time is at least 15 minutes. 13. The method of claim 9 , wherein the heating is conducted in an inert atmosphere. 14. The method of claim 9 , wherein the heating is conducted in a reducing atmosphere.
Manufacture or treatment of nanostructures · CPC title
Electronic properties · CPC title
Size or surface area · CPC title
Chemistry & Metallurgy · mapped topic
Purity · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.