Hydrocracking catalyst for hydrocarbon oil, method for producing hydrocracking catalyst, and method for hydrocracking hydrocarbon oil with hydrocracking catalyst
US-9221036-B2 · Dec 29, 2015 · US
US9512371B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9512371-B2 |
| Application number | US-201013377023-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 16, 2010 |
| Priority date | Aug 21, 2009 |
| Publication date | Dec 6, 2016 |
| Grant date | Dec 6, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A support for hydrocracking catalyst of hydrocarbon oil, which comprises a modified zeolite obtained by incorporating titanium into a faujasite-type zeolite, wherein the modified zeolite satisfies conditions (a) to (e) as described, and to a hydrocracking catalyst employing the support and a method for hydrocracking of hydrocarbon oil containing aromatics using the catalyst.
Opening claim text (preview).
The invention claimed is: 1. A support for hydrocracking catalyst of hydrocarbon oil, which consists essentially of a modified zeolite obtained by incorporating titanium into an ultra stabilized Y zeolite (USY), wherein the modified zeolite satisfies the followings (a) to (e): (a) the modified zeolite has a titanium content of 1-17% by mass in terms of metal oxide amount, (b) the modified zeolite contains aluminum and silicon in an Al/Si atomic ratio of 0.14-0.35, (c) the modified zeolite has a lattice constant of 24.36-24.48 Å, (d) the modified zeolite has a degree of crystallinity of 30-95%, and (e) the modified zeolite has a specific surface area of 500-850 m 2 /g. 2. A catalyst for hydrocracking of hydrocarbon oil, which comprises: the support according to claim 1 ; and at least one selected from Group 8 metals and Group 6 metals of the long-form periodic table in an amount of 0.5-30% by mass in terms of metal oxide amount based on the catalyst. 3. A method for hydrocracking of hydrocarbon oil, which comprises hydrocracking hydrocarbon oil which has a boiling-point range of 120-380° C. and comprises aromatic hydrocarbon compounds in an amount of 30-100% by mass, by contacting the hydrocarbon oil with the hydrocracking catalyst according to claim 2 .
Aromatics or polyaromatics · CPC title
Impregnation · CPC title
Acid treatment · CPC title
Molybdenum · CPC title
Titanium; Oxides or hydroxides thereof · CPC title