Polypropylene resin foamed particles, polypropylene resin in-mold foam molded article, and method for producing same
US-9493622-B2 · Nov 15, 2016 · US
US9505857B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9505857-B2 |
| Application number | US-201214005108-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 16, 2012 |
| Priority date | Mar 17, 2011 |
| Publication date | Nov 29, 2016 |
| Grant date | Nov 29, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided are pre-expanded polypropylene resin particles having a dimensional expansion coefficient of 1.5% or more determined with a thermomechanical analyzer at a constant compressive load of 1 mg during heating from 30° C. to 100° C. at a temperature increase rate of 10° C./min. Using the pre-expanded polypropylene resin particles can yield an in-mold foam molded product of polypropylene resin having few wrinkles and small dimensional shrinkage without pretreatment such as internal pressure application or compression packing during packing the pre-expanded particles in a mold for in-mold foam molding.
Opening claim text (preview).
The invention claimed is: 1. Pre-expanded polypropylene resin particles comprising a polypropylene resin as a substrate resin, the resin particles having an average particle weight of 3 mg/particle or less, and the pre-expanded particles having a dimensional expansion coefficient of 1.5% or more determined with a thermomechanical analyzer at a constant compressive load of 0.1 g during heating from 30° C. to 100° C. at a temperature increase rate of 10° C./min. 2. An in-mold foam molded product of polypropylene resin obtained by in-mold foam molding of the pre-expanded polypropylene resin particles according to claim 1 , without internal pressure application.
characterized by the use of several polymeric components · CPC title
by impregnating polymer particles with the blowing agent · CPC title
Saturated hydrocarbons, e.g. butane; Unspecified hydrocarbons · CPC title
by sintering expandable particles · CPC title
using several expanding {or moulding} steps · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.