Insulated electrical wire and production method therefor
US-2024052199-A1 · Feb 15, 2024 · US
US9458355B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9458355-B2 |
| Application number | US-201313971003-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 20, 2013 |
| Priority date | Aug 21, 2012 |
| Publication date | Oct 4, 2016 |
| Grant date | Oct 4, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A polyimide resin produced by heating a polyamic acid resulting from the reaction of a tetracarboxylic acid dianhydride component and a diamine component in N,N,N′,N′-tetramethylurea.
Opening claim text (preview).
What is claimed is: 1. A method of producing a polyimide coating, consisting essentially of heating a polyimide precursor coating formed by coating on a base substance, wherein the polyimide precursor coating consists of a polyamic acid solution in N,N,N′,N′-tetramethylurea, the polyamic acid solution consists of a solution resulting from the reaction of reactants consisting of a tetracarboxylic acid dianhydride component and a diamine component in N,N,N′,N′-tetramethylurea, wherein the tetracarboxylic acid dianhydride component consists of one or more compounds selected from the group consisting of pyromellitic acid dianhydride, 3,3′,4,4′-biphenyl tetracarboxylic acid dianhydride, 2,3,3′,4′-biphenyl tetracarboxylic acid dianhydride, 3,3′,4,4′-benzophenone tetracarboxylic acid dianhydride, and 3,3′,4,4′-diphenylsulfonetetracarboxylic acid dianhydride, and the polyimide precursor coating is heated at a temperature from 120° C. to 350° C. 2. The method of producing a polyimide coating according to claim 1 , wherein the amount of N,N,N′,N′-tetramethylurea is from 20 to 2000 parts by mass based on 100 parts by mass of total amount of the tetracarboxylic acid dianhydride component and the diamine component.
characterised by the solvent(s) used · CPC title
derived from polyamines and polycarboxylic acids · CPC title
Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors · CPC title
characterised by the process itself, e.g. steps, continuous · CPC title