Methods for operating polyethylene reactor systems
US-2024392119-A1 · Nov 28, 2024 · US
US9447210B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9447210-B2 |
| Application number | US-201313871638-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 26, 2013 |
| Priority date | Oct 29, 2010 |
| Publication date | Sep 20, 2016 |
| Grant date | Sep 20, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided are an olefin composition, filler and an optoelectronic device. One illustrative olefin composition may be effectively used as a filling material for various optoelectronic devices.
Opening claim text (preview).
What is claimed is: 1. A filler that comprises an olefin polymer that has at least one hydrolyzable group and at least one hydrolyzed product of the hydrolyzable group hydrolyzed in the presence of a basic hydrolysis catalyst which is an organic amine compound, wherein the filler has a gel fraction that is measured according to ASTM D 2765 after being kept in water of 90° C. for 18 hours is from 5% to 60%, wherein the olefin polymer has an index of a hydrolysable group in a range from 0.01 to 1.5, and an index of the hydrolyzed product of the hydrolysable group in a range from 0.01 to 1.5, the indices being measured by Fourier transform infrared spectrometry, wherein the filler has a 90-degree peel strength that is measured after being compressed on a glass substrate using a laminator at 150° C. for 10 minutes is 100 N/15 mm or more, and wherein the amount of the basic hydrolysis catalyst remaining in the filler is in the range from 300 ppm to 6,000 ppm. 2. The filler according to claim 1 , wherein the filler has a gel fraction that is measured according to ASTM D 2765 after being kept in water of 90° C. for 18 hours is from 10% to 50%.
Polyethylene · CPC title
Materials of encapsulations · CPC title
Ethene · CPC title
with aliphatic 1-olefins containing one carbon-to-carbon double bond · CPC title
Photovoltaic [PV] energy · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.