Topical protective polymerized nanoparticles in an active or bioactive array, methods for preparing same and uses thereof
US-2015374610-A1 · Dec 31, 2015 · US
US9428596B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9428596-B2 |
| Application number | US-201214369657-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 27, 2012 |
| Priority date | Dec 28, 2011 |
| Publication date | Aug 30, 2016 |
| Grant date | Aug 30, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of production of modified conjugated diene-based rubber comprising a steps of using, as a polymerization initiator, an alkali metalated aromatic compound which has three or more carbon atoms which are directly bonded to alkali metal atoms and aromatic rings in one molecule so as to polymerize a monomer which contains at least a conjugated diene compound and reacting a compound of the following general formula (I) with an active ends of the obtained polymer is provided. (In the general formula (I), any one of R 1 and R 10 to R 18 is an atom or reactive group which can react with the active ends of said polymer or a hydrocarbon group which includes either of the same, the remaining among R 1 and R 10 to R 18 and R 2 to R 9 are respectively independently a hydrogen atom, alkyl group, or aryl group, and “j”, “k”, “m”, and “n” are integers of 0 to 100.)
Opening claim text (preview).
The invention claimed is: 1. A method of production of modified conjugated diene-based rubber, comprising: a first step of using, as a polymerization initiator, an alkali metalated aromatic compound which has three or more carbon atoms which are directly bonded to alkali metal atoms and aromatic rings in one molecule so as to polymerize a monomer which contains at least a conjugated diene compound and obtain a conjugated diene-based rubber which has active ends; and a second step of reacting a compound of the following formula (I) with the active ends of said conjugated diene-based rubber which has active ends, wherein, in the formula (I), any one of R 1 and R 10 to R 18 is an atom or reactive group which can react with the active ends of said conjugated diene-based rubber which has active ends or a hydrocarbon group which contains one of either said atom or said reactive group, while the remaining among R 1 and R 10 to R 18 are respectively independently a hydrogen atom, C 1 to C 10 alkyl group, or C 6 to C 12 aryl group, R 2 to R 9 are respectively independently a hydrogen atom, C 1 to C 10 alkyl group, or C 6 to C 12 aryl group, “j”, “k”, “m”, and “n” are respectively independently integers of 0 to 100. 2. The method of production of modified conjugated diene-based rubber as set forth in claim 1 , wherein, in said first step, a monomer which contains an aromatic vinyl compound in addition to said conjugated diene compound is copolymerized. 3. The method of production of modified conjugated diene-based rubber as set forth in claim 1 , wherein said alkali metalated aromatic compound is one which is obtained by making an aromatic compound which has three or more carbon atoms which are directly bonded to aromatic rings in one molecule react with an organic alkali metal compound. 4. The method of production of modified conjugated diene-based rubber as set forth in claim 3 , wherein said aromatic compound which has three or more carbon atoms which are directly bonded to aromatic rings in one molecule is an aromatic compound of the following formula (II), wherein, in the formula (II), R 19 to R 26 are respectively independently a hydrogen atom or C 1 to C 10 alkyl group and three or more of R 19 to R 26 are C 1 to C 10 alkyl groups, “p” is an integer of 0 to 5 and, when “p” is 2 or more, regardless of the structure of the above formula (II), three or more present benzene rings may be condensed at any positions with each other. 5. The method of production of modified conjugated diene-based rubber as set forth in claim 1 wherein, in said formula (I), said atom or reactive group which can react with the active ends of the conjugated diene-based rubber which has active ends is a halogen atom, vinyl group, alkoxyl group, amino group, or epoxy group. 6. A modified conjugated diene-based rubber which is obtained by the method of production as set forth in claim 1 . 7. A rubber composition containing a rubber ingredient which contains the modified conjugated diene-based rubber as set forth in claim 6 in 100 parts by weight and silica in 10 to 200 parts by weight. 8. The rubber composition as set forth in claim 7 which further contains a cross-linking agent. 9. A rubber cross-linked product obtained by cross-linking the rubber composition as set forth in claim 8 . 10. A tire which contains the rubber cross-linked product as set forth in claim 9 .
conjugated · CPC title
Incorporating silicon atoms into the molecule · CPC title
an alkali metal bound to a cyclic carbon · CPC title
Silica · CPC title
taking place solely at one end or both ends of the polymer backbone, i.e. not in the side or lateral chains · CPC title