Thin thermally strengthened glass cover panel for vehicle frame assembly and related method
US-2020406837-A1 · Dec 31, 2020 · US
US9415626B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9415626-B2 |
| Application number | US-201514627176-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 20, 2015 |
| Priority date | Nov 30, 2011 |
| Publication date | Aug 16, 2016 |
| Grant date | Aug 16, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A deco glass panel including a mother substrate formed of glass, a glass powder layer welded on the mother substrate and a rear surface pattern disposed on a rear surface of the mother substrate, wherein the rear surface pattern is located within an outline of the glass powder layer when viewed from the front surface of the mother substrate.
Opening claim text (preview).
What is claimed is: 1. A deco glass panel, comprising: a mother substrate formed of glass; a glass powder layer welded on the mother substrate; and a rear surface pattern disposed on a rear surface of the mother substrate, wherein the rear surface pattern is located within an outline of the glass powder layer when viewed from the front surface of the mother substrate, wherein the glass powder comprises, by weight, 11-20% SiO 2 , 30-35% ZnO, 15-20% B 2 O 3 , 10-18% Na 2 O, 1-5% Al 2 O 3 , 1-4% ZrO 2 , 1-4% CaO, 0.05-0.25% Fe 2 O 3 and 0.001-0.004% MnO and other impurities. 2. The deco glass panel of claim 1 , wherein the glass powder further comprises, by weight, 0.05-0.25% Fe 2 O 3 and 0.001-0.004% MnO. 3. The deco glass panel of claim 1 , wherein a film layer is additionally provided on a rear surface of the rear surface pattern. 4. A deco glass panel, comprising: a mother substrate formed of glass; a glass powder layer welded on the mother substrate; and a film disposed on a rear surface of the mother substrate, wherein the film has a prescribed surface pattern with a different color from a ground color of the film and the rear surface pattern has the same shape of the glass powder layer, wherein the glass powder comprises, by weight, 11-20% SiO 2 , 30-35% ZnO, 15-20% B 2 O 2 , 10-18% Na 2 O, 1-5% Al 2 O 3 , 1-4% ZrO 2 , 1-4% CaO, 0.05-0.25% Fe 2 O 3 and 0.001-0.004% MnO and other impurities. 5. The deco glass panel of claim 4 , wherein the prescribed surface pattern is formed to be within an outline of the glass powder layer when viewed from an upper surface of the mother substrate.
including ceramic, glass, porcelain or quartz layer · CPC title
Masking · CPC title
Decorative coatings · CPC title
containing zinc · CPC title
Designs imitating three-dimensional [3D] effects · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.