Composition for soft materials, and soft material
US-2015361209-A1 · Dec 17, 2015 · US
US9409999B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9409999-B2 |
| Application number | US-201114004849-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 5, 2011 |
| Priority date | Mar 14, 2011 |
| Publication date | Aug 9, 2016 |
| Grant date | Aug 9, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention aims to provide a method of producing a hydrophilic modified polyrotaxane, which enables production of a hydrophilic modified polyrotaxane excellent in storage stability in an industrially advantageous way. The present invention provides a method of producing a hydrophilic modified polyrotaxane, comprising: a hydrophilic modification step of preparing a solution of a hydrophilic modified polyrotaxane by modifying all or part of hydroxy groups on a cyclodextrin of a polyrotaxane with hydrophilic modifying groups, the polyrotaxane containing the cyclodextrin, a polyethylene glycol included in the cavities of the cyclodextrin molecules in a skewered manner, and a capping group that is placed at each end of the polyethylene glycol and prevents dissociation of the cyclodextrin molecules from the polyethylene glycol; and a drying step in which the prepared solution of the hydrophilic modified polyrotaxane is formed into a thin film state and dried.
Opening claim text (preview).
The invention claimed is: 1. A method of producing a hydrophilic modified polyrotaxane, comprising: a hydrophilic modification step of preparing a solution of a hydrophilic modified polyrotaxane by modifying all or part of hydroxy groups on a cyclodextrin of a polyrotaxane with hydrophilic modifying groups, the polyrotaxane containing the cyclodextrin, a polyethylene glycol included in the cavities of the cyclodextrin molecules in a skewered manner, and a capping group that is placed at each end of the polyethylene glycol and prevents dissociation of the cyclodextrin molecules from the polyethylene glycol; and a drying step in which the prepared solution of the hydrophilic modified polyrotaxane is formed into a thin film state and dried, a thickness of a thin film formed being 0.1 to 2 mm. 2. The method of producing a hydrophilic modified polyrotaxane according to claim 1 , wherein the polyethylene glycol has a weight average molecular weight of 1,000 to 500,000. 3. The method of producing a hydrophilic modified polyrotaxane according to claim 1 , wherein the drying step is carried out at a drying temperature of 70° C. to 200° C. 4. The method of producing a hydrophilic modified polyrotaxane according to the claim 1 , wherein the pressure in the dryer system in the drying step is equal to or lower than an atmospheric pressure. 5. The method of producing a hydrophilic modified polyrotaxane according to the claim 1 , wherein a drying time in the drying step is two minutes or shorter.
Inclusion compounds, i.e. host-guest compounds, e.g. polyrotaxanes · CPC title
cyclic · CPC title
Cyclodextrin; Derivatives thereof · CPC title
End-capping · CPC title
Manufacture of films or sheets · CPC title