Method for producing lithium secondary cell

US9406967B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9406967-B2
Application numberUS-201013993135-A
CountryUS
Kind codeB2
Filing dateDec 17, 2010
Priority dateDec 17, 2010
Publication dateAug 2, 2016
Grant dateAug 2, 2016

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Provided is a method for producing a lithium secondary cell with which the concentrated precipitation of metal impurities at the negative electrode is inhibited and short circuiting is unlikely to occur. The production method includes, assembling together the positive electrode, the separator, and the negative electrode, and then impregnating the assembly with the nonaqueous electrolyte; charging the assembly within 1 min so that a maximum achieved potential of the positive electrode becomes 3.2 V or more with respect to the redox potential of lithium; allowing the assembly to stand for 10 min or less after the charging has ended; and discharging the assembly within 1 min after the standing step.

First claim

Opening claim text (preview).

The invention claimed is: 1. A method for producing a lithium secondary cell provided with a positive electrode having a positive electrode active material made of a lithium-containing complex oxide, a negative electrode having a negative electrode active material capable of absorbing and releasing lithium ions, a separator interposed between the positive electrode and the negative electrode, and a nonaqueous electrolyte impregnated in the positive electrode, the negative electrode, and the separator, comprising: assembling together the positive electrode, the separator, and the negative electrode, and then impregnating the assembly with the nonaqueous electrolyte; preliminary charging the assembly within 1 min so that a maximum achieved potential of the positive electrode becomes 3.2 V or more with respect to the redox potential of lithium; allowing the assembly to stand for 10 min or less after the preliminary charging has ended; preliminary discharging the assembly within 1 min after the standing step; and thereafter charging the assembly to a predetermined capacity. 2. The method for producing a lithium secondary cell according to claim 1 , further comprising: allowing the assembly to stand after the preliminary discharging has ended, wherein the preliminary charging step, the standing step after the preliminary charging, the preliminary discharging step, and the standing step after the preliminary discharging are repeated one, two or more times before the assembly is charged to a predetermined capacity. 3. The method for producing a lithium secondary cell according to claim 2 , wherein the positive electrode active material is made of a lithium-containing complex oxide including at least manganese, cobalt, and nickel, and the preliminary charging time is longer than the preliminary discharging time. 4. The method for producing a lithium secondary cell according to claim 2 , wherein the preliminary charging step, the standing step after the preliminary charging, the preliminary discharging step, and the standing step after the preliminary discharging are repeated ten or more times. 5. The method for producing a lithium secondary cell according to claim 1 , wherein the assembly is allowed to stand for 5 min or less in the standing step after the preliminary charging. 6. The method for producing a lithium secondary cell according to claim 1 , wherein an electric current equal to or higher than 1 C is supplied during the preliminary charging and/or preliminary discharging. 7. The method for producing a lithium secondary cell according to claim 1 , wherein the preliminary charging is performed for 1 sec to 10 sec in the preliminary charging step. 8. The method for producing a lithium secondary cell according to 1 , wherein the preliminary discharging is performed for 1 sec to 10 sec in the preliminary discharging step. 9. The method for producing a lithium secondary cell according to claim 1 , wherein a maximum achieved potential of the negative electrode is set to be 3.2 V or less with respect to the redox potential of lithium in the preliminary discharging step. 10. The method for producing a lithium secondary cell according to claim 1 , further comprising: allowing the assembly to stand for 30 min or more after all of the preliminary charging step, the standing step after the preliminary charging, and the preliminary discharging step, have ended; and charging the assembly in excess of 1 min.

Assignees

Inventors

Classifications

  • Manufacturing or production processes characterised by the final manufactured product · CPC title

  • Cross-Sectional Technologies · mapped topic

  • Cross-Sectional Technologies · mapped topic

  • H01M4/139Primary

    Processes of manufacture · CPC title

  • Cross-Sectional Technologies · mapped topic

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9406967B2 cover?
Provided is a method for producing a lithium secondary cell with which the concentrated precipitation of metal impurities at the negative electrode is inhibited and short circuiting is unlikely to occur. The production method includes, assembling together the positive electrode, the separator, and the negative electrode, and then impregnating the assembly with the nonaqueous electrolyte; chargi…
Who is the assignee on this patent?
Fujimaki Hisataka, Hojo Katsuyuki, Hagino Tomotaka, and 4 more
What technology area does this patent fall under?
Primary CPC classification H01M4/139. Mapped technology areas include Electricity.
When was this patent published?
Publication date Tue Aug 02 2016 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).