Electrical steel sheet and method for manufacturing same
US-12163066-B2 · Dec 10, 2024 · US
US9406437B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9406437-B2 |
| Application number | US-201113814532-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 5, 2011 |
| Priority date | Aug 6, 2010 |
| Publication date | Aug 2, 2016 |
| Grant date | Aug 2, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A grain oriented electrical steel sheet has thickness of forsterite film at bottom portions of grooves formed on a surface of the steel sheet is ≧0.3 μm, groove frequency is ≦20%, abundance ratio of grooves crystal grains directly beneath themselves, each crystal grain having orientation deviating from Goss orientation by ≧10° and grain size ≧5 μm, total tension exerted on the steel sheet in the rolling direction by the forsterite film and tension coating is ≧10.0 MPa, total tension exerted on the steel sheet in a direction perpendicular to the rolling direction by the forsterite film and tension coating is ≧5.0 MPa and total tension satisfies 1.0≦A/B≦5.0, where A is total tension exerted in rolling direction by forsterite film and tension coating, and B is total tension exerted in direction perpendicular to rolling direction by forsterite film and tension coating.
Opening claim text (preview).
The invention claimed is: 1. A grain oriented electrical steel sheet comprising: a forsterite film, tension coating on a surface of the steel sheet; and grooves for magnetic domain refinement on the surface of the steel sheet, wherein 1) a thickness of the forsterite film at bottom portions of the grooves is 0.3 μm or more, 2) groove frequency is 20% or less, the groove frequency being a ratio of the number of grooves, each groove having crystal grains directly beneath itself, each crystal grain having an orientation deviating from a Goss orientation by 10° or more and a grain size of 5 μm or more to the number of all grooves, and 3) total tension exerted on the steel sheet in a rolling direction by the forsterite film and the tension coating is 10.0 MPa or more, a total tension exerted on the steel sheet in a direction perpendicular to the rolling direction by the forsterite film and the tension coating is 5.0 MPa or more, and total tensions satisfy: 1.0≦ A/B≦ 5.0, where A is total tension exerted in the rolling direction by the forsterite film and the tension coating, and B is total tension exerted in a direction perpendicular to the rolling direction by the forsterite film and the tension coating.
with insulating coating · CPC title
Rolling special iron alloys {, e.g. stainless steel} · CPC title
Composite web or sheet · CPC title
Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00) · CPC title