Pivotal door for adjusting the position of and gaining access to a grinding roller of a pulverizer mill
US-2024226912-A9 · Jul 11, 2024 · US
US9358549B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9358549-B2 |
| Application number | US-201214004538-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 16, 2012 |
| Priority date | Apr 19, 2011 |
| Publication date | Jun 7, 2016 |
| Grant date | Jun 7, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed is a method for manufacturing a carbide for reinforcing rubber articles that is capable of effectively utilizing polymer waste. The method includes the steps of mixing a carbide, obtained by thermal decomposition or incomplete combustion of polymer waste and pulverized by grinding, with carbon black to obtain a mixture of the carbide and the carbon black, and granulating the mixture using a granulating machine at a rotation speed of 70 rpm to 130 rpm.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing a carbide for reinforcing rubber articles comprising the steps of: mixing a carbide, obtained by thermal decomposition or incomplete combustion of polymer waste and pulverized by grinding, with carbon black to obtain a mixture of the carbide and the carbon black; and granulating the mixture in an amount range of 1 kg to 2 kg using a granulating machine at a rotation speed of 70 rpm to 130 rpm and for a time range of 110 s to 130 s. 2. The method for manufacturing a carbide for reinforcing rubber articles according to claim 1 , wherein a mixture mass ratio of the carbide to the carbon black is in a range of 1/99 to 50/50. 3. The method for manufacturing a carbide for reinforcing rubber articles according to claim 2 , wherein the carbon black is a powdered material or a ground product of a granular material. 4. The method for manufacturing a carbide for reinforcing rubber articles according to claim 1 , wherein the carbon black is a powdered material or a ground product of a granular material. 5. The method for manufacturing a carbide for reinforcing rubber articles according to claim 1 , wherein the rotation speed is 110 rpm to 130 rpm. 6. The method for manufacturing a carbide for reinforcing rubber articles according to claim 1 , wherein the carbide is obtained by thermal decomposition or incomplete combustion of polymer waste at a temperature in the range of 300° C. to 600° C.
Pyrolysis, carbonisation or auto-combustion reactions · CPC title
Auxiliary methods or auxiliary devices or accessories specially adapted for crushing or disintegrating not provided for in preceding groups or not specially adapted to apparatus covered by a single preceding group ({specially adapted for grain mills B02C11/00;} separating or sorting in general B03, B04, B07) · CPC title
specially adapted for specific materials not otherwise provided for · CPC title
Carbon black · CPC title
Carbides · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.