High-strength cold-rolled steel sheet having excellent surface quality and low material variation, and method for manufacturing same
US-2024384366-A1 · Nov 21, 2024 · US
US9330839B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9330839-B2 |
| Application number | US-201113814357-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 3, 2011 |
| Priority date | Aug 6, 2010 |
| Publication date | May 3, 2016 |
| Grant date | May 3, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A grain oriented electrical steel sheet is subjected to magnetic domain refining treatment by electron beam irradiation and exhibits excellent low-noise properties when assembled as an actual transformer, in which a ratio (Wa/Wb) of a film thickness (Wa) of the forsierite film on a strain-introduced side of the steel sheet to a film thickness (Wb) of the forsierite film on a non-strain-introduced side of the steel sheet is 0.5 or higher, a magnetic domain discontinuous portion in a surface of the steel sheet on the strain-introduced side has an average width of 150 to 300 μm, and a magnetic domain discontinuous portion in a surface of the steel sheet on the non-strain-introduced side has an average width of 250 to 500 μm.
Opening claim text (preview).
The invention claimed is: 1. A grain oriented electrical steel sheet comprising a forsterite film formed on a surface thereof, being subjected to strain introduction by an electron beam and having a magnetic flux density B 8 of 1.92 T or higher, wherein a ratio (Wa/Wb) of a film thickness of the forsterite film on a strain-introduced side of the steel sheet (Wa) to a film thickness of the forsterite film on a non-strain-introduced side of the steel sheet (Wb) is 0.5 or higher, and wherein a magnetic domain discontinuous portion in a surface of the steel sheet on the strain-introduced side has an average width in a direction at right angles to a longitudinal direction of the magnetic domain discontinuous portion of 150 to 300 μm, and a magnetic domain discontinuous portion in a surface of the steel sheet on the non-strain-introduced side has an average width in a direction at right angles to a longitudinal direction of the magnetic domain discontinuous portion of 250 to 500 μm. 2. The grain oriented electrical steel sheet according to claim 1 , wherein Wa/Wb is 0.5 to 0.9.
during manufacturing of plates or strips (C21D8/12 takes precedence) · CPC title
Recycling · CPC title
containing silicon · CPC title
containing Ni (C21D6/004 takes precedence) · CPC title
Final recrystallisation annealing · CPC title