Thermoplastic Resin Composition and Molded Article Manufactured Therefrom
US-2024376301-A1 · Nov 14, 2024 · US
US9267010B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9267010-B2 |
| Application number | US-201214366829-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 20, 2012 |
| Priority date | Dec 20, 2011 |
| Publication date | Feb 23, 2016 |
| Grant date | Feb 23, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The instant invention provides a rotomolding composition. The a rotomolding composition comprises at least 95 percent by weight of a thermoplastic polymer; and from 0.1 to 3 percent by weight of metal oxide lamellae; wherein the rotomolding composition is characterized by at least one of the following properties: (a) having a retention at elongation at break of at least 85 percent after 4000 hours of accelerated aging; or (b) having a ductility improvement of at least 50 percent relative to a similar composition free of said metal oxide lamellae.
Opening claim text (preview).
We claim: 1. A rotomolding composition comprising: at least 95 percent by weight of a thermoplastic polymer; and from 0.1 to 3 percent by weight of iron oxide lamellae having a purity of at least 99 percent or greater, a hardness in the range of 6 to 6.5 Mohs, and an average aspect ratio (long axis/thickness) in the range of from 2 to 30 and wherein said iron oxide lamella has an average size diameter (long axis) in the range of from 2 to 20 μM; wherein said rotomolding composition is characterized by at least one of the following properties: (a) having a retention at elongation at break of at least 85 percent after 4000 hours of accelerated aging; or (b) having a ductility improvement of at least 50 percent relative to a similar composition free of said iron oxide lamellae. 2. The rotomolding composition according to claim 1 , wherein said rotomolding composition is further characterized by having a tensile modulus (2%) improvement of at least 10 percent relative to a similar composition free of said iron oxide lamellae. 3. The rotomolding composition of claim 1 , wherein said thermoplastic polymer is an ethylene based polymer or a propylene based polymer.