Process for adding a coupling agent to raw stock

US9254584B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9254584-B2
Application numberUS-201013147052-A
CountryUS
Kind codeB2
Filing dateJan 29, 2010
Priority dateJan 30, 2009
Publication dateFeb 9, 2016
Grant dateFeb 9, 2016

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The invention relates to a process for manufacturing composite material which contains fiber based and polymer based material, wherein the manufacture includes a preliminary treatment process to form a raw stock mixture. According to the invention, the preliminary treatment process includes a hot-cold mixing device which comprises at least a heating stage, and that raw stock, which contains lignin-free material, and a coupling agent are fed to the mixing device to form the raw stock mixture, and adhesion between fiber based and polymer based substances of the raw stock is ameliorated by the coupling agent.

First claim

Opening claim text (preview).

The invention claimed is: 1. A process for manufacturing composite material which contains a wood fiber based lignin-free material and a polymer based material, wherein the process for manufacturing includes a preliminary treatment process to form agglomerates from a raw stock mixture, wherein the preliminary treatment process includes a hot-cold mixing device which comprises at least a heating stage and a cooling stage, the hot-cold mixing device provides a temperature of above 180° C., a dwell time of at least 15 minutes, a contact area and a mixing rate that provides reaction between a raw stock and a coupling agent, wherein the preliminary treatment process comprises feeding the coupling agent, the raw stock containing the wood fiber based lignin-free material, and the polymer based material to the hot-cold mixing device to form the raw stock mixture, heating the raw stock mixture in the heating stage of the hot-cold mixing device to the temperature of above 180° C. for a dwell time of at least 15 minutes wherein adhesion between the fiber based lignin-free material and the polymer based material of the raw stock is ameliorated by the coupling agent, the temperature, the dwell time, the mixing rate and the contact area, cooling and mixing the raw stock mixture in the cooling stage of the hot-cold mixing device, and forming the agglomerates from the raw stock mixture in the hot-cold mixing device. 2. The process according to claim 1 , further comprising forming the raw stock mixture in the mixing device to a temperature of above 185° C. 3. The process according to claim 1 , wherein the raw stock comprises recycling material which contains the wood fiber based lignin-free material and/or the polymer based material. 4. The process according to claim 1 , wherein the raw stock comprises adhesive laminate waste. 5. The process according to claim 1 , further comprising crushing the raw stock to a predetermined particle size before conducting it to the mixing device. 6. The process according to claim 1 , further comprising feeding additional plastic to the mixing device. 7. The process according to claim 1 , further comprising feeding additive to the mixing device. 8. The process according to claim 1 , wherein the coupling agent comprises organic material which contains maleic anhydrides. 9. The process according to claim 1 , wherein the coupling agent is selected from the group of MAPE, MAPP and mixtures thereof. 10. The process according to claim 5 , wherein the particle size of the raw stock is between 1 and 10 mm.

Assignees

Inventors

Classifications

  • Mixing the material with binding agent (mixing in general B01F) · CPC title

  • Tarpaulins · CPC title

  • Plastics recycling; Rubber recycling · CPC title

  • B29B17/00Primary

    Recovery of plastics or other constituents of waste material containing plastics; ({volume reduction of waste plastics, e.g. by mechanical compacting or melting disposal of solid waste B09B;} chemical recovery C08J11/00) · CPC title

  • Layered products · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9254584B2 cover?
The invention relates to a process for manufacturing composite material which contains fiber based and polymer based material, wherein the manufacture includes a preliminary treatment process to form a raw stock mixture. According to the invention, the preliminary treatment process includes a hot-cold mixing device which comprises at least a heating stage, and that raw stock, which contains lig…
Who is the assignee on this patent?
Lehtinen Liisa, Peltola Piia, Laaksonen Risto, and 1 more
What technology area does this patent fall under?
Primary CPC classification B29B17/00. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Feb 09 2016 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.