Aluminum alloy casting and production method thereof

US9243312B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9243312-B2
Application numberUS-201013391445-A
CountryUS
Kind codeB2
Filing dateJul 27, 2010
Priority dateSep 10, 2009
Publication dateJan 26, 2016
Grant dateJan 26, 2016

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

There is provided an aluminum alloy casting consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities, or consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance being Al and unavoidable impurities, and containing eutectic Si grains having an aspect ratio of 2.0 or smaller and an average grain size of 1.0 micrometer or smaller. There is also provided an automotive part formed with the aluminum alloy casting and a production method of the aluminum alloy casting.

First claim

Opening claim text (preview).

The invention claimed is: 1. An aluminum alloy cast member consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities and containing eutectic Si grains having an aspect ratio of 2.0 or smaller and an average grain size of 1.0 micrometer or smaller. 2. An aluminum alloy cast member consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance being Al and unavoidable impurities and containing eutectic Si grains having an aspect ratio of 2.0 or smaller and an average grain size of 1.0 micrometer or smaller. 3. An aluminum alloy cast member according to claim 1 , wherein the content of said Si is 8.0 to 10.0 mass %; and the content of said Mg is 1.0 to 4.0 mass %. 4. An automotive part comprising an aluminum alloy casting according to claim 1 . 5. A method of producing an aluminum alloy casting according to claim 1 , comprising: preparing a molten aluminum alloy consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities; and injecting the molten aluminum alloy into a casting mold to thereby cast the molten aluminum alloy under the condition that an average flow rate of the molten aluminum alloy in the casting mold is 12 m/s or higher. 6. An aluminum alloy cast member according to claim 2 , wherein the content of said Si is 8.0 to 10.0 mass %; and the content of said Mg is 1.0 to 4.0 mass %. 7. An automotive part comprising an aluminum alloy casting according to claim 2 . 8. A method of producing an aluminum alloy casting according to claim 2 , comprising: preparing a molten aluminum alloy consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance being Al and unavoidable impurities; and injecting the molten aluminum alloy into a casting mold to thereby cast the molten aluminum alloy under the condition that an average flow rate of the molten aluminum alloy in the casting mold is 12 m/s or higher.

Assignees

Inventors

Classifications

  • with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C · CPC title

  • Modified aluminium-silicon alloys · CPC title

  • C22C21/02Primary

    with silicon as the next major constituent · CPC title

  • Pressure die casting or injection die casting, i.e. casting in which the metal is forced into a mould under high pressure · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9243312B2 cover?
There is provided an aluminum alloy casting consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn and the balance being Al and unavoidable impurities, or consisting essentially of 7.0 to 11.5 mass % of Si, 0.9 to 4.0 mass % of Mg, 0.1 to 0.65 mass % of Fe, 0.1 to 0.8 mass % of Mn, 0.3 to 1.0 mass % of Cu and the balance be…
Who is the assignee on this patent?
Nagaishi Yusuke, Nakagawa Shigeyuki, Itakura Koji, and 4 more
What technology area does this patent fall under?
Primary CPC classification C22C21/02. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Jan 26 2016 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).