Communication electric wire
US-2024105362-A1 · Mar 28, 2024 · US
US9165697B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9165697-B2 |
| Application number | US-201314084391-A |
| Country | US |
| Kind code | B2 |
| Filing date | Nov 19, 2013 |
| Priority date | Nov 20, 2012 |
| Publication date | Oct 20, 2015 |
| Grant date | Oct 20, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A peroxide crosslinked resin composition includes a base polymer (A) including 50 to 90% by mass of a first copolymer component (a1) including one of or a mixture of two or more first ethylene α-olefin copolymers having a density of 0.864 to 0.890 g/cm 3 , a melt flow rate (MFR) of 1 to 5 g/10 min, and a melting point of not higher than 90 degrees Celsius, and 10 to 50% by mass of a second copolymer component (a2) including one of or a mixture of two or more second ethylene α-olefin copolymers having a melt flow rate (MFR) of not smaller than 30 g/10 min, and a melting point of 55 to 80 degrees Celsius, an inorganic filler (B) added in a ratio of from 80 parts to 150 parts by mass with respect to 100 parts by mass of the base polymer (A), and a peroxide crosslinker (C).
Opening claim text (preview).
What is claimed is: 1. A peroxide crosslinked resin composition, including: a base polymer (A) including 50 to 90% by mass of a first copolymer component (a1) comprising one of or a mixture of two or more first ethylene α-olefin copolymers having a density of 0.864 to 0.890 g/cm 3 , a melt flow rate (MFR) of 1 to 5 g/10 min, and a melting point of not higher than 90 degrees Celsius, and 10 to 50% by mass of a second copolymer component (a2) comprising one of or a mixture of two or more second ethylene α-olefin copolymers having a melt flow rate (MFR) of not smaller than 30 g/10 min, and a melting point of 55 to 80 degrees Celsius; an inorganic filler (B) added in an amount of from 80 parts to 150 parts by mass with respect to 100 parts by mass of the base polymer (A); and a peroxide crosslinker (C). 2. The peroxide crosslinked resin composition according to claim 1 , wherein the inorganic filler (B) comprises a mean grain diameter of 0.8 to 2.5 μm. 3. An electric wire, comprising: a conductor; and an insulator formed around an outer periphery of the conductor by coating with the peroxide crosslinked resin composition according to claim 1 . 4. A cable, comprising: the electric wire according to claim 3 .
Crosslinking · CPC title
use in electrical wires or wirecoating · CPC title
from alkenes · CPC title
containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure · CPC title
Additives being defined by their diameter · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.