Power cable comprising interpolymer compositions and methods for making the same
US-9208923-B2 · Dec 8, 2015 · US
US9109065B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9109065-B2 |
| Application number | US-201214350056-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 12, 2012 |
| Priority date | Oct 13, 2011 |
| Publication date | Aug 18, 2015 |
| Grant date | Aug 18, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Objects of the invention are to obtain ethylene copolymers which have excellent rubber elasticity even without being crosslinked and maintain sufficient shaping processability even when filled with significantly large amounts of additives, and to provide methods for producing with good productivity films or sheets having flexibility and high stretchability. The invention is directed to an ethylene copolymer (X) including structural units derived from a component [A], a component [B] and a component [C] which are ethylene [A], an α-olefin of 3 to 20 carbon atoms [B] and a polyene and/or a cyclic olefin [C]. In the ethylene copolymer, (1) the content of structural units derived from the ethylene [A] is in the range of 50 to 90 mol % in 100 mol % of all the structural units in the copolymer (X); (2) the content of structural units derived from at least one polyene and/or the cyclic olefin [C] is in the range of 1.0 to 5.0 mol % in 100 mol % of all the structural units in the copolymer (X); and (3) the intrinsic viscosity [η] of the ethylene copolymer (X) as measured at 135° C. in a decalin solution is in the range of 7.8 to 13.0 dl/g. The invention also concerns with a composition including the ethylene copolymer (X), and uses.
Opening claim text (preview).
The invention claimed is: 1. An ethylene copolymer (X) , which satisfies the following (i) and (ii), comprising structural units derived from a component [A], a component [B] and a component [C] which are ethylene [A], an α-olefin of 3 to 20 carbon atoms [B] and a polyene and/or a cyclic olefin [C], (1) the content of structural units derived from the ethylene [A] being in the range of 50 to 90 mol% in 100 mol% of all the structural units in the copolymer (X); (2) the content of…
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Related publications grouped by family.
Free tools are coming soon. Tell us what you want to track and we'll notify you.
Answers are generated from the same data shown on this page.