Method for Producing Water-Absorbing Polymer Particles with High Swelling Rate and High Centrifuge Retention Capacity with Simultaneously High Permeability of the Swollen Gel Bed
US-2015376318-A1 · Dec 31, 2015 · US
US8975339B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-8975339-B2 |
| Application number | US-67885608-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 8, 2008 |
| Priority date | Oct 9, 2007 |
| Publication date | Mar 10, 2015 |
| Grant date | Mar 10, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a surface treatment method for a water-absorbent resin having excellent production efficiency, absorption capacity against pressure, fluid permeability or the like. Provided is a method for the surface treatment of a water-absorbent resin which comprises a) a step for mixing 0.1 to 20 parts by weight of an acid group-containing radically polymerizable compound and 5 to 20 parts by weight of water, relative to 100 parts by weight of a water-absorbent resin; and b) a step for polymerizing the acid group-containing radically polymerizable compound, wherein neutralization ratio of the acid group-containing radically polymerizable compound is 0 to 60% by mol, and is lower than neutralization ratio of the water-absorbent resin.
Opening claim text (preview).
The invention claimed is: 1. A surface-treated water-absorbent resin obtained by a method comprising: a) a step for mixing 0.1 to 20 parts by weight of an acid group-containing radically polymerizable compound and 5 to 20 parts by weight of water, relative to 100 parts by weight of a water-absorbent resin; and b) a step for polymerizing the acid group-containing radically polymerizable compound, wherein neutralization ratio of the acid group-containing radically polymerizable…
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Related publications grouped by family.
Free tools are coming soon. Tell us what you want to track and we'll notify you.
Answers are generated from the same data shown on this page.