Positively chargeable single-layer electrophotographic photosensitive member, process cartridge, and image forming apparatus
US-2016349635-A1 · Dec 1, 2016 · US
US8974992B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-8974992-B2 |
| Application number | US-201313871489-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 26, 2013 |
| Priority date | Nov 2, 2012 |
| Publication date | Mar 10, 2015 |
| Grant date | Mar 10, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is an electrophotographic photoreceptor including an electroconductive substrate, an undercoat layer that is provided on the electroconductive substrate, contains a binder resin, metal oxide particles and an electron accepting compound having an acidic group and has an AC impedance of from 1×10 5 Ω to 1×10 8 Ω under the measurement condition in which a temperature is 22° C., a humidity is 50% RH, an AC voltage is ±1 V, and a frequency is 1 Hz and an AC impedance of from 1×10 3 Ω to 1×10 8 Ω under the measurement condition in which a temperature is 22° C., a humidity is 50% RH, an AC voltage is ±1 V, and a frequency is 100 Hz, and a photosensitive layer that is provided on the undercoat layer.
Opening claim text (preview).
What is claimed is: 1. An electrophotographic photoreceptor comprising: an electroconductive substrate; an undercoat layer that is provided on the electroconductive substrate, contains a binder resin, metal oxide particles and an electron accepting compound having an acidic group and has an AC impedance of from 1×10 5 Ω to 1×10 8 Ω under the measurement condition in which a temperature is 22° C., a humidity is 50% RH, an AC voltage is ±1 V, and a frequency is 1 Hz and an AC impe…
Physics · mapped topic
Physics · mapped topic
Physics · mapped topic
Related publications grouped by family.
Free tools are coming soon. Tell us what you want to track and we'll notify you.
Answers are generated from the same data shown on this page.