Method for extracting a refractory metal from an ore, a concentrate or a waste product
US-2022364205-A1 · Nov 17, 2022 · US
US8945491B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-8945491-B2 |
| Application number | US-201314010500-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 26, 2013 |
| Priority date | Nov 14, 2012 |
| Publication date | Feb 3, 2015 |
| Grant date | Feb 3, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for extracting vanadium from shale, the method including: a) grinding the shale into fine powders, mixing the fine powders with an additive in a mass ratio of 1:0.04-0.12 to yield a mixture, heating the mixture to a temperature of between 850 and 950° C. at a heating rate of 5-9° C./min, and baking the mixture for between 30 and 90 min; b) immersing the product in water and acid respectively to yield a first solution and a second solution, combining the two solutions, and performing ion exchange adsorption on the combined solution using a styrene-divinylbenzene based macroporous anion-exchange resin; and c) performing desorption, purification, and precipitation to yield poly ammonium vanadate, and calcining the poly ammonium vanadate at a temperature of between 450 and 530° C. for between 20 and 50 min to yield V 2 O 5 .
Opening claim text (preview).
The invention claimed is: 1. A method for extracting vanadium from shale, the method comprising the following steps: a) grinding the shale into fine powders, mixing the fine powders with an additive in a mass ratio of 1:0.04-0.12 to yield a mixture, heating the mixture to a temperature of between 850 and 950° C. at a heating rate of 5-9° C./min, and baking the mixture for between 30 and 90 min; b) immersing a product resulting from the baking in step a) in water to yield a first…