Method And System For Utilizing Radio-Opaque Fillers In Multiple Layers Of Golf Balls
US-2024424351-A1 · Dec 26, 2024 · US
US8932152B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-8932152-B2 |
| Application number | US-201213645136-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 4, 2012 |
| Priority date | Oct 6, 2011 |
| Publication date | Jan 13, 2015 |
| Grant date | Jan 13, 2015 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A center of a golf ball is formed from a composition having a flexural modulus from 150-450 MPa, a maximum loss factor (tan δ) between −20 and 0° C. of 0.08 or less, a rebound resilience of 55% or more, and a slab hardness ranging from 40-60 in Shore D hardness. The center composition includes, as a resin component, 30 to 70 mass % of (A) a modified polyester elastomer having a Shore A hardness of 95 or less; 70-30 mass % of (B) a binary ionomer resin having a Shore D hardness of 65 or more, a flexural modulus of 300 MPa or more, and a melt flow rate (190° C., 2.16 kg) of 1.0 g/10 min or more; and 0-50 mass % of (C) a thermoplastic resin other than (A) and (B) components (provided that a total content of (A), (B), and (C) components is 100 mass %).
Opening claim text (preview).
The invention claimed is: 1. A golf ball having a center, a cover, and at least one intermediate layer disposed between the center and the cover, wherein the center is formed from a center composition having a flexural modulus ranging from 150 MPa to 450 MPa, a maximum loss factor (tan δ) between −20° C. and 0° C. of 0.08 or less, a rebound resilience of 55% or more, and a slab hardness ranging from 40 to 60 in Shore D hardness, and the center composition comprises, as a resin comp…
Human Necessities · mapped topic
Human Necessities · mapped topic
Human Necessities · mapped topic
Human Necessities · mapped topic
Human Necessities · mapped topic
Related publications grouped by family.
Free tools are coming soon. Tell us what you want to track and we'll notify you.
Answers are generated from the same data shown on this page.