Hot forming of curved mirrors without the need for a mandrel
US-2024018030-A1 · Jan 18, 2024 · US
US2025389871A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2025389871-A1 |
| Application number | US-202519238702-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jun 16, 2025 |
| Priority date | Jun 21, 2024 |
| Publication date | Dec 25, 2025 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A film mirror laminate ( 1 ) includes a substrate film ( 2 ), a metal reflective layer ( 3 ), a reflection adjustment layer ( 4 ), and a water-repellent layer ( 5 ) in order toward one side in a thickness direction. The reflection adjustment layer ( 4 ) includes a silicon oxide layer ( 43 ), and the water-repellent layer ( 5 ) is disposed on one surface in the thickness direction of the silicon oxide layer ( 43 ). Further, a water contact angle in one surface in the thickness direction of the water-repellent layer ( 5 ) is 110° or more.
Opening claim text (preview).
1 . A film mirror laminate comprising: a substrate film, a metal reflective layer, a reflection adjustment layer, and a water-repellent layer in order toward one side in a thickness direction, wherein the reflection adjustment layer includes a silicon oxide layer, the water-repellent layer is disposed on one surface in the thickness direction of the silicon oxide layer, and a water contact angle in one surface in the thickness direction of the water-repellent layer is 110° or more. 2 . The film mirror laminate according to claim 1 , wherein a reflection rate of a visible ray at a wavelength of 360 to 740 nm irradiated from one side in the thickness direction of the film mirror laminate is 95.0% or more. 3 . The film mirror laminate according to claim 1 , wherein the metal reflective layer includes at least one metal selected from the group consisting of aluminum (Al), zinc (Zn), lead (Pb), copper (Cu), and silver (Ag). 4 . The film mirror laminate according to claim 1 , wherein the reflection adjustment layer includes a low refractive index layer, a high refractive index layer, and the silicon oxide layer in order toward one side in the thickness direction. 5 . The film mirror laminate according to claim 1 , wherein the silicon oxide layer has a thickness of 50 nm or less. 6 . The film mirror laminate according to claim 1 , wherein the water-repellent layer is a dry coating layer. 7 . A mirror member comprising: a support substrate, a pressure-sensitive adhesive layer, and the film mirror laminate according to claim 1 in order toward one side in a thickness direction.
Protective coatings, e.g. hard coatings · CPC title
the reflecting layers comprising a single metallic layer with one or more dielectric layers · CPC title
with a refractive index gradient (rugate filters G02B5/289) · CPC title
Coatings for keeping optical surfaces clean, e.g. hydrophobic or photo-catalytic films (G02B1/16 takes precedence) · CPC title
having a single reflecting layer (G02B5/0883, G02B5/0891 take precedence) · CPC title