Solid-state electrochemical cell
US-2024429457-A1 · Dec 26, 2024 · US
US2025385242A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2025385242-A1 |
| Application number | US-202519215338-A |
| Country | US |
| Kind code | A1 |
| Filing date | May 22, 2025 |
| Priority date | Jun 13, 2024 |
| Publication date | Dec 18, 2025 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing a secondary battery electrode includes: drying an electrode paste formed on a surface of a current collector; after drying the electrode paste, baking the electrode paste at a higher temperature than during the drying; and after baking the electrode paste, bending the current collector around a roller surface such that the surface of the current collector on which the electrode paste is formed is disposed at an outer side.
Opening claim text (preview).
What is claimed is: 1 . A method for producing a secondary battery electrode, the method comprising: drying an electrode paste formed on a surface of a current collector; after drying the electrode paste, baking the electrode paste at a higher temperature than during the drying; and after baking the electrode paste, bending the current collector around a roller surface such that the surface of the current collector on which the electrode paste is formed is disposed at an outer side. 2 . The method for producing a secondary battery electrode of claim 1 , wherein, when baking the electrode paste, a baking temperature and a baking time satisfy the following equations: Y≥− 8 X+ 1220 100 ≤X≤ 150 wherein, in the equations, X is the baking temperature in degrees Celsius and Y is the baking time in minutes. 3 . The method for producing a secondary battery electrode of claim 1 , wherein a roller having a roll diameter of 40 mm or greater is employed in the bending. 4 . The method for producing a secondary battery electrode of claim 1 , wherein a thickness of the electrode paste formed on the current collector is from 150 μm to 500 μm. 5 . The method for producing a secondary battery electrode of claim 1 , wherein, in the bending, cracks are imparted having a depth that is 10% or greater with respect to a thickness of the electrode paste formed on the current collector and that is a depth not reaching the current collector.
Processes of manufacture · CPC title
Rolling or calendering · CPC title
by coating on electrode collectors · CPC title
involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis · CPC title
Energy storage using batteries · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.