Processing hard rock lithium minerals or other materials to produce lithium materials and byproducts converted from a sodium sulfate intermediate product
US-2024425381-A1 · Dec 26, 2024 · US
US2025154626A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2025154626-A1 |
| Application number | US-202418943040-A |
| Country | US |
| Kind code | A1 |
| Filing date | Nov 11, 2024 |
| Priority date | Nov 10, 2023 |
| Publication date | May 15, 2025 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Described herein is a method for purifying black mass of a battery, comprising providing processed cathode or anode black mass, and bringing processed black mass into contact with a basic mixture, wherein the basic mixture comprises at least one alcohol and at least one alkoxide.
Opening claim text (preview).
1 . A method for purifying black mass of a battery, comprising: providing processed cathode or anode black mass; and bringing processed black mass into contact with a basic mixture; wherein the basic mixture comprises at least one alcohol and at least one alkoxide. 2 . The method of claim 1 , wherein the at least one alcohol is a C 3 -C 8 alcohol. 3 . The method of claim 1 , wherein the at least one alkoxide is an alkali metal alkoxide or a transition metal alkoxide. 4 . The method of claim 1 , wherein the at least one alkoxide is a Li-alkoxide. 5 . The method of claim 1 , wherein the basic mixture has a pH value in the range of greater than 7.5. 6 . The method of claim 1 , wherein the ratio of the at least one alcohol to the at least one alkoxide is in the range from 99:1 to 8:2. 7 . The method of claim 1 , wherein the black mass is dry black mass. 8 . The method of claim 1 , wherein the processed black mass and the basic mixture are wet-crushed together. 9 . The method of claim 1 , further comprising a mechanical separation of the black mass and the basic mixture. 10 . A method of utilizing a basic mixture comprising at least one alcohol and at least one alkoxide for purifying black mass. 11 . The method of claim 10 , wherein the basic mixture comprises at least one Li-alkoxide. 12 . The method of claim 10 , wherein the at least one alkoxide is an alkali metal alkoxide or a transition metal alkoxide. 13 . The method of claim 10 , wherein the at least one alkoxide is a Li-alkoxide. 14 . The method of claim 10 , wherein the basic mixture has a pH value in the range of greater than 7.5. 15 . The method of claim 10 , wherein the ratio of the at least one alcohol to the at least one alkoxide is in the range from 99:1 to 8:2. 16 . The method of claim 10 , wherein the black mass is dry black mass. 17 . The method of claim 10 , wherein the processed black mass and the basic mixture are wet-crushed together. 18 . The method of claim 10 , further comprising a mechanical separation of the black mass and the basic mixture. 19 . The method of claim 10 , wherein the black mass is processed cathode or anode black mass.
Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof · CPC title
Wet processes · CPC title
Reclaiming serviceable parts of waste accumulators · CPC title
Recycling of batteries or fuel cells · CPC title