Degradable polymeric compositions and articles comprising same
US-2024425683-A1 · Dec 26, 2024 · US
US2024254294A9 · US · A9
| Field | Value |
|---|---|
| Publication number | US-2024254294-A9 |
| Application number | US-202117360040-A |
| Country | US |
| Kind code | A9 |
| Filing date | Jun 28, 2021 |
| Priority date | Dec 28, 2018 |
| Publication date | Aug 1, 2024 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A water-soluble film is provided that is capable of achieving deformation resistance during pouch storage as well as excellent water solubility of the film and excellent reduction in undissolved residues. A water-soluble film includes a polyvinyl alcohol-based resin, wherein a crystal long period Ds obtained from an X-ray profile obtained by small-angle X-ray scattering measurement in a water/methanol mixed solvent (volume ratio: 2/8) is from 10.0 to 30.0 nm and a rate of increase (DS−Da)/Da of the crystal long period Ds to a crystal long period Da obtained by small-angle X-ray scattering measurement before immersion in the solvent is 30% or more and 130% or less.
Opening claim text (preview).
1 . A water-soluble film comprising a polyvinyl alcohol-based resin, wherein a crystal long period Ds obtained from an X-ray profile obtained by small-angle X-ray scattering measurement in a water/methanol mixed solvent (volume ratio: 2/8) is from 10.0 to 30.0 nm and a rate of increase (DS−Da)/Da of the crystal long period Ds to a crystal long period Da obtained by small-angle X-ray scattering measurement before immersion in the solvent is 30% or more and 130% or less. 2 . The water-soluble film according to claim 1 , wherein the crystal long period Da of the water-soluble film obtained by small-angle X-ray scattering measurement before immersion in the solvent is from 9.0 to 15.0 nm. 3 . A package comprising: the water-soluble polyvinyl alcohol film according to claim 1 or 2 and a chemical contained using the water-soluble polyvinyl alcohol film. 4 . The package according to any one of claims 1 through 3 , wherein the chemical is a pesticide, a detergent, or a germicide. 5 . The package according to claim 3 or 4 , wherein the chemical is in a liquid form.
Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids · CPC title
water-soluble · CPC title
Films or sheets · CPC title
Stepwise homogeneous crosslinking of one polymer with one crosslinking system, e.g. partial curing · CPC title
Polymers characterized by their physical structure · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.