Method for manufacturing a polyacrylonitrile-sulfur composite material
US-10096834-B2 · Oct 9, 2018 · US
US2022340693A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2022340693-A1 |
| Application number | US-202017763839-A |
| Country | US |
| Kind code | A1 |
| Filing date | Sep 14, 2020 |
| Priority date | Sep 27, 2019 |
| Publication date | Oct 27, 2022 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention provides a method of producing sulfur-modified polyacrylonitrile, including: a step (1) of heating polyacrylonitrile and elemental sulfur in a rotating-type heating container including a discharge pipe and a sulfur vapor recovery unit while rotating the rotating-type heating container; a step (2) of liquefying a sulfur vapor by the sulfur vapor recovery unit while discharging hydrogen sulfide generated in the heating step; and a step (3) of returning the liquefied sulfur to a mixture of the sulfur and the polyacrylonitrile of the step (1).
Opening claim text (preview).
1 . A method of producing sulfur-modified polyacrylonitrile, comprising: a step (1) of heating polyacrylonitrile and elemental sulfur in a rotating-type heating container comprising a discharge pipe and a sulfur vapor recovery unit while rotating the rotating-type heating container; a step (2) of liquefying a sulfur vapor by the sulfur vapor recovery unit while discharging hydrogen sulfide generated in the heating step; and a step (3) of returning the liquefied sulfur to a mixture of the sulfur and the polyacrylonitrile of the step (1). 2 . The method of producing sulfur-modified polyacrylonitrile according to claim 1 , wherein a ratio between the polyacrylonitrile and the elemental sulfur is as follows: 100 parts by mass to 1,500 parts by mass of the elemental sulfur with respect to 100 parts by mass of the polyacrylonitrile. 3 . The method of producing sulfur-modified polyacrylonitrile according to claim 1 , wherein the polyacrylonitrile and the elemental sulfur each have a particle diameter of from 1 μm to 1,000 μm in terms of an average particle diameter. 4 . The method of producing sulfur-modified polyacrylonitrile according to claim 1 , wherein the polyacrylonitrile and the elemental sulfur each have a particle diameter of from 1 μm to 1,000 μm in terms of an average particle diameter.
specially adapted for lithium-ion capacitors, e.g. for lithium-doping or for intercalation · CPC title
Carbon pastes or blends; Binders or additives therein · CPC title
Homopolymers or copolymers of acrylonitrile (C08L55/02 takes precedence) · CPC title
specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34) · CPC title
Acrylonitrile · CPC title