Chute turning restriction mechanism
US-8967358-B2 · Mar 3, 2015 · US
US2022314491A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2022314491-A1 |
| Application number | US-202117365296-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jul 1, 2021 |
| Priority date | Apr 1, 2021 |
| Publication date | Oct 6, 2022 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Methods for modifying a recycled fine powder of concrete and uses thereof. A method for modifying a recycled fine powder can include: crushing a collected waste concrete block step by step with a crusher, grinding with a ball mill, and passing through a 100-mesh sieve, to obtain a recycled fine powder with d50 of 13.5 μm; placing the obtained recycled fine powder in a dry environment at a high temperature, drying, then taking out, and cooling to room temperature; preparing tannic acid solutions with different concentrations, mixing the cooled recycled fine powder with the prepared tannic acid solutions, and continuously stirring by a glass rod.
Opening claim text (preview).
What is claimed is: 1 . A method for modifying a recycled fine powder of concrete, comprising: crushing a collected waste concrete block step by step with a crusher, grinding with a ball mill, and passing through a 100-mesh sieve, to obtain said recycled fine powder with d50 of 13.5 μm; placing said recycled fine powder in a dry environment at a high temperature, drying, then taking out, and cooling to room temperature; and preparing a plurality of tannic acid solutions with different concentrations, mixing said recycled fine powder with said plurality of tannic acid solutions, and continuously stirring by a glass rod. 2 . The method of claim 1 , wherein the drying is performed at a temperature of 105° C. for 2 hours. 3 . The method of claim 1 , wherein the tannic acid solutions have a mass fraction (accounting for the mass of water) of 0%, 0.3% and 0.5%, respectively. 4 . The method of claim 1 , wherein continuously stirring by said glass rod is performed for 2 minutes. 5 . The method of claim 1 , wherein said plurality of tannic acid solutions are analytical reagents with a purity of ≥95%. 6 . A method for using the recycled fine powder modified by the method of claim 1 in a concrete, comprising using the recycled fine powder modified by the plurality of tannic acid solutions with different concentrations to replace cement with a replacement rate of 10%.
from waste building materials, e.g. waste asbestos-cement products, demolition waste · CPC title
from building or ceramic industry · CPC title
Polysaccharides or derivatives thereof {(C04B24/243 takes precedence)} · CPC title
Methods for mixing (B28C5/386, B28C5/402 take precedence) · CPC title
with stirrers sweeping through the materials {, e.g. with incorporated feeding or discharging means or with oscillating stirrers} · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.