Iron oxyhydroxynitrate having phosphoric acid anion-adsorbed surface, preparation method therefor, cathode comprising iron oxyhydroxynitrate having phosphoric acid anion-adsorbed surface for lithium secondary battery, and lithium secondary battery comprising same

US2022223860A1 · US · A1

Patent metadata
FieldValue
Publication numberUS-2022223860-A1
Application numberUS-202017608336-A
CountryUS
Kind codeA1
Filing dateJul 1, 2020
Priority dateAug 13, 2019
Publication dateJul 14, 2022
Grant date

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed is a modified iron oxyhydroxynitrate including iron oxyhydroxynitrate and hydrogen phosphate ions adsorbed on a surface thereof. Also disclosed is a method for preparing the same, a positive electrode for a lithium secondary battery including the modified iron oxyhydroxynitrate as a positive electrode additive, and a lithium secondary battery including the same.

First claim

Opening claim text (preview).

1 . A modified iron oxyhydroxynitrate comprising: an iron oxyhydroxynitrate of the following Formula 1 FeO(NO 3 ) x (OH) 1−x wherein 0<x<1; and  [Formula 1] hydrogen phosphate ions (HPO 4 2− ) adsorbed on a surface of the iron oxyhydroxynitrate. 2 . The modified iron oxyhydroxynitrate according to claim 1 , wherein the hydrogen phosphate ions are adsorbed as a monolayer on the surface of the iron oxyhydroxynitrate. 3 . The modified iron oxyhydroxynitrate according to claim 1 , wherein the iron oxyhydroxynitrate of Formula 1 is present as particles having an average particle diameter of 1 μm to 200 μm. 4 . The modified iron oxyhydroxynitrate according to claim 1 , wherein the modified iron oxyhydroxynitrate is suitable as an additive for a positive electrode for a lithium secondary battery. 5 . A method for preparing an iron oxyhydroxynitrate with hydrogen phosphate ions (HPO 4 2− ) adsorbed on its surface comprising the steps of: (1) preparing a Fe(NO 3 ) 3 .9H 2 O solution by dissolving Fe(NO 3 ) 3 .9H 2 O in a mixed solvent comprising an aqueous solvent and an organic solvent; (2) drying the Fe(NO 3 ) 3 .9H 2 O solution to obtain iron oxyhydroxynitrate of the following Formula 1; (3) preparing an aqueous phosphoric acid solution having a pH of 6 to 12; (4) preparing a mixed solution by mixing the iron oxyhydroxynitrate of Formula 1 obtained in step (2) with the aqueous phosphoric acid solution having a pH of 6 to 12; and (5) recovering and drying solid material after a reaction of the mixed solution is completed: FeO(NO 3 ) x (OH) 1−x wherein 0<x<1.  [Formula 1] 6 . The method for preparing the iron oxyhydroxynitrate with hydrogen phosphate ions adsorbed on its surface according to claim 5 , wherein a concentration of the Fe(NO 3 ) 3 .9H 2 O solution in step (1) is 0.5 to 2.5 M. 7 . The method for preparing the iron oxyhydroxynitrate with hydrogen phosphate ions adsorbed on its surface according to claim 5 , wherein the aqueous solvent and the organic solvent of step (1) are mixed in a weight ratio of 30:70 to 70:30. 8 . The method for preparing the iron oxyhydroxynitrate with hydrogen phosphate ions adsorbed on its surface according to claim 5 , wherein a concentration of the aqueous phosphoric acid solution in step (3) is 1×10 −5 to 1×10 −1 M. 9 . The method for preparing the iron oxyhydroxynitrate with hydrogen phosphate ions adsorbed on its surface according to claim 5 , wherein the iron oxyhydroxynitrate of Formula 1 is present in an amount of 10 to 80% by weight with respect to a total weight of the mixed solution in step (4). 10 . The method for preparing the iron oxyhydroxynitrate with hydrogen phosphate ions adsorbed on its surface according to claim 5 , further comprising: after step (4), a step of re-adjusting the pH of the mixed solution to 6 to 12. 11 . A positive electrode for a lithium secondary battery comprising a positive electrode current collector; and a positive electrode active material layer located on at least one side of the positive electrode current collector, wherein the positive electrode active material layer comprises a positive electrode active material, an electrically conductive material, a binder and an additive, wherein the binder contains a carboxylate group, and wherein the additive comprises the modified iron oxyhydroxynitrate of claim 1 . 12 . The positive electrode for a lithium secondary battery according to claim 11 , wherein the additive is present in an amount of 0.1 to 40 parts by weight relative to 100 parts by weight of base solid material included in the positive electrode active material layer. 13 . The positive electrode for a lithium secondary battery according to claim 11 , wherein the positive electrode active material comprises at least one selected from the group consisting of elemental sulfur (S 8 ), organic sulfur compounds, and sulfur-carbon composite. 14 . A lithium secondary battery comprising a positive electrode; a negative electrode; a separator interposed between the positive electrode and the negative electrode; and an electrolyte solution, wherein the positive electrode is the positive electrode of claim 11 . 15 . The lithium secondary battery according to claim 14 , wherein the lithium secondary battery is a lithium-sulfur battery. 16 . The positive electrode for a lithium secondary battery according to claim 11 , wherein the binder is at least one selected from the group consisting of poly(vinyl)acetate, poly(methyl methacrylate), poly(ethyl acrylate), carboxymethyl cellulose, polyethylene glycol diacrylate, blends thereof, and copolymers thereof.

Assignees

Inventors

Classifications

  • Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries · CPC title

  • Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof · CPC title

  • Micrometer sized, i.e. from 1-100 micrometer · CPC title

  • obtained by SEM · CPC title

  • Compounds containing iron, with or without oxygen or hydrogen, and containing two or more other elements · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US2022223860A1 cover?
Disclosed is a modified iron oxyhydroxynitrate including iron oxyhydroxynitrate and hydrogen phosphate ions adsorbed on a surface thereof. Also disclosed is a method for preparing the same, a positive electrode for a lithium secondary battery including the modified iron oxyhydroxynitrate as a positive electrode additive, and a lithium secondary battery including the same.
Who is the assignee on this patent?
Lg Energy Solution Ltd
What technology area does this patent fall under?
Primary CPC classification H01M4/628. Mapped technology areas include Electricity.
When was this patent published?
Publication date Thu Jul 14 2022 00:00:00 GMT+0000 (Coordinated Universal Time) (A1). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).