Method for manufacturing lithium secondary battery
US-2019221881-A1 · Jul 18, 2019 · US
US2022102731A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2022102731-A1 |
| Application number | US-202017422583-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jan 16, 2020 |
| Priority date | Jan 16, 2019 |
| Publication date | Mar 31, 2022 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A lithium secondary battery is disclosed herein. In some embodiments, a lithium secondary battery includes: a battery case having an interior region, a separator, wherein the separator divides the interior region into a first region and a second region, a positive electrode formed in the first region and including a positive electrode active material and positive electrode current collector particles; and a negative electrode formed in the second region and including a negative electrode active material and negative electrode current collector particles.
Opening claim text (preview).
1 . A lithium secondary battery comprising: a battery case having an interior region; a separator, wherein the separator divides the interior region into a first region and a second region; a positive electrode formed in the first region and including a positive electrode active material and positive electrode current collector particles; and a negative electrode formed in the second region and including a negative electrode active material and negative electrode current collector particles. 2 . The lithium secondary battery of claim 1 , wherein the positive electrode has a porosity of 20% to 30%. 3 . The lithium secondary battery of claim 1 , wherein the negative electrode has a porosity of 25% to 35%. 4 . The lithium secondary battery of claim 1 , wherein the positive electrode current collector particles are present at 1 wt % to 15 wt %, relative to the total weight of the positive electrode, and wherein the negative electrode current collector particles are present at 1 wt % to 15 wt %, relative to the total weight of the negative electrode. 5 . The lithium secondary battery of claim 1 , wherein the positive electrode current collector particles and the negative electrode current collector particles each independently have an average particle diameter (D 50 ) of 0.5 μm to 3 μm. 6 . The lithium secondary battery of claim 1 , wherein the positive electrode current collector particles and the negative electrode current collector particles each independently include at least one selected from the group consisting of aluminum, copper, stainless steel, nickel, and titanium. 7 . The lithium secondary battery of claim 1 , wherein the positive electrode active material includes a first positive electrode active material and a second positive electrode active material, wherein the first positive electrode active material has a larger average particle diameter (D 50 ) than the second positive electrode active material. 8 . The lithium secondary battery of claim 7 , wherein the first positive electrode active material has an average particle diameter (D 50 ) of 10 μm to 18 μm, and the second positive electrode active material has an average particle diameter (D 50 ) of 2 μm to 8 μm. 9 . A method of producing a lithium secondary battery, comprising: injecting a first mixture into a first region of a battery case and injecting a second mixture into a second region of the battery case, wherein the first region and second region are part of an interior region of the battery case, wherein a separator separates the first region from the second region, wherein the first mixture includes a positive electrode active material and positive electrode current collector particles, and wherein the second mixture includes a negative electrode active material and negative electrode current collector particles; and after the injection of the first and second mixtures, rolling the battery case while applying pressure. 10 . The method of claim 9 , wherein the first mixture and the second mixture are each independently injected in the form of a slurry or powder into the battery case. 11 . The method of claim 9 , further comprising: during the injection of the first mixture and the second mixture, vibrating the battery case. 12 . The method of claim 9 , further comprising: after the injection of the first and second mixtures, drying the battery case. 13 . The method of claim 12 , wherein the drying of the battery case occurs prior to or simultaneously with the rolling. 14 . The method of claim 9 , further comprising injecting an electrolyte into the interior region of the battery case after the battery case has been rolled. 15 . The method of claim 14 , further comprising: after the injection of the electrolyte, sealing the battery case by evacuating air bubbles from the interior region of the battery case.
Pouches or flexible bags · CPC title
Physical characteristics, e.g. porosity, surface area · CPC title
Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence) · CPC title
Compression means other than compression means for stacks of electrodes and separators · CPC title
Manufacturing or production processes characterised by the final manufactured product · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.