Manufacturing method of aluminum-based article with multi-angle visual color change characteristics
US-2024344229-A1 · Oct 17, 2024 · US
US2021147997A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2021147997-A1 |
| Application number | US-202117160220-A |
| Country | US |
| Kind code | A1 |
| Filing date | Jan 27, 2021 |
| Priority date | Jul 31, 2018 |
| Publication date | May 20, 2021 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present disclosure relates to an aluminum member including a mother material containing aluminum or an aluminum alloy, and an anodic oxide film on the surface of the mother material. The anodic oxide film has a barrier layer on the surface of the mother material, and a porous layer on the barrier layer), and the BET specific surface area of the anodic oxide film is 0.1 to 10.0 m 2 /g.
Opening claim text (preview).
What is claimed is: 1 . An aluminum member comprising: a mother material containing aluminum or an aluminum alloy; and an anodic oxide film on a surface of the mother material, wherein the anodic oxide film has a barrier layer on a surface of the mother material, and a porous layer on the barrier layer, and a BET specific surface area of the anodic oxide film is 0.1 to 10.0 m 2 /g. 2 . The aluminum member according to claim 1 , wherein a Hunter whiteness of the aluminum member, measured from a surface side of the anodic oxide film, is 65 or more. 3 . A method of manufacturing the aluminum member according to claim 1 , comprising: a step of preparing a mother material comprising aluminum or an aluminum alloy; and a step of performing an anodic oxidation treatment on the mother material in an electrolytic solution including: (a) a first acid being an inorganic acid or a salt of the first acid; and (b) at least one second acid selected from the group consisting of diphosphoric acid, triphosphoric acid, and polyphosphoric acid, or a salt of the second acid. 4 . The method of manufacturing the aluminum member according to claim 3 , wherein in the step of performing the anodic oxidation treatment, a concentration of the first acid or a salt of the first acid in the electrolytic solution is 0.005 to 7.0 mol·dm −3 , and a concentration of the second acid or a salt of the second acid in the electrolytic solution is 0.005 to 10.0 mol·dm −3 . 5 . The method of manufacturing the aluminum member according to claim 3 , wherein in the step of performing the anodic oxidation treatment, a current density is 2 to 150 mA·cm −2 , and an electrolysis time is 10 to 700 minutes.
Related publications grouped by family.
Answers are generated from the same data shown on this page.