Biodegradable magnesium alloys, methods of manufacture thereof and articles comprising the same
US-2016194738-A1 · Jul 7, 2016 · US
US2019060995A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2019060995-A1 |
| Application number | US-201816117324-A |
| Country | US |
| Kind code | A1 |
| Filing date | Aug 30, 2018 |
| Priority date | Aug 31, 2017 |
| Publication date | Feb 28, 2019 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A raw material for thixomolding includes a magnesium-based alloy powder which contains calcium in an amount of 0.2 mass % or more and 5 mass % or less and aluminum in an amount of 2.5 mass % or more and 12 mass % or less, wherein the magnesium-based alloy powder includes an oxide layer which has an average thickness of 30 nm or more and 100 nm or less and contains at least one of calcium and aluminum as an outermost layer. The average dendrite secondary arm spacing of crystal structures of the magnesium-based alloy powder is preferably 5 μm or less.
Opening claim text (preview).
What is claimed is: 1 . A raw material for thixomolding, comprising a magnesium-based alloy powder which contains calcium in an amount of 0.2 mass % or more and 5 mass % or less and aluminum in an amount of 2.5 mass % or more and 12 mass % or less, wherein the magnesium-based alloy powder includes an oxide layer which has an average thickness of 30 nm or more and 100 nm or less and contains at least one of calcium and aluminum as an outermost layer. 2 . The raw material for thixomolding according to claim 1 , wherein the average dendrite secondary arm spacing of crystal structures of the magnesium-based alloy powder is 5 μm or less. 3 . The raw material for thixomolding according to claim 1 , wherein the minimum particle diameter of the magnesium-based alloy powder is 0.5 mm or more. 4 . A method for producing a raw material for thixomolding, which is a method for producing the raw material for thixomolding according to claim 1 , comprising producing the magnesium-based alloy powder by a spinning water atomization method. 5 . A method for producing a raw material for thixomolding, which is a method for producing the raw material for thixomolding according to claim 2 , comprising producing the magnesium-based alloy powder by a spinning water atomization method. 6 . A method for producing a raw material for thixomolding, which is a method for producing the raw material for thixomolding according to claim 3 , comprising producing the magnesium-based alloy powder by a spinning water atomization method. 7 . A molded body, comprising the raw material for thixomolding according to claim 1 . 8 . A molded body, comprising the raw material for thixomolding according to claim 2 . 9 . A molded body, comprising the raw material for thixomolding according to claim 3 .
Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10) · CPC title
Metallic powder characterised by the size or surface area of the particles · CPC title
with aluminium as the next major constituent · CPC title
atomising using a fluid (using centrifugal force B22F9/10) · CPC title
using screws · CPC title