Plug for rolling of seamless steel pipe, method for manufacturing the same and method for manufacturing seamless steel pipe using the same
US-2015217349-A1 · Aug 6, 2015 · US
US2018354008A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2018354008-A1 |
| Application number | US-201615762821-A |
| Country | US |
| Kind code | A1 |
| Filing date | Aug 12, 2016 |
| Priority date | Sep 25, 2015 |
| Publication date | Dec 13, 2018 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A piercer plug with increased life and a method of manufacturing it are provided. The piercer plug 1 includes a tip portion 2 and a trunk portion 3 made of the same material as the tip portion 2 and continuous to the tip portion 2. The trunk portion 3 includes a cylindrical portion 5 having a hole used for attaching a bar. The tip portion 2 is harder than the cylindrical portion 5.
Opening claim text (preview).
1 . A piercer plug comprising: a tip portion; and a trunk portion made of the same material as the tip portion and continuous to the tip portion, wherein the trunk portion includes a cylindrical portion having a hole used for attaching a bar, and the tip portion is harder than the cylindrical portion. 2 . The piercer plug according to claim 1 , further comprising: a coating formed on a surface of the piercer plug. 3 . A method of manufacturing a piercer plug, the method comprising: preparing a piercer plug including a tip portion and a trunk portion made of the same material as the tip portion and continuous to the tip portion; and heating the piercer plug such that a temperature of the tip portion is not lower than an austenite transformation temperature and a temperature of a cylindrical portion included in the trunk portion and having a hole used for attaching a bar is lower than the austenite transformation temperature. 4 . The method of manufacturing a piercer plug according to claim 3 , further comprising: forming a coating on a surface of the piercer plug before the heating.
with copper · CPC title
Mandrels for metal tube rolling mills, e.g. mandrels of the types used in the methods covered by group B21B17/00; Accessories or auxiliary means therefor {; Construction of, or alloys for, mandrels or plugs} · CPC title
with molybdenum or tungsten · CPC title
containing Cr and Ni · CPC title
Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.