Castable Ce-Based Magnets
US-2024379263-A1 · Nov 14, 2024 · US
US2018291484A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2018291484-A1 |
| Application number | US-201615767523-A |
| Country | US |
| Kind code | A1 |
| Filing date | Oct 12, 2016 |
| Priority date | Nov 17, 2015 |
| Publication date | Oct 11, 2018 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention relates to a copper-nickel-zinc alloy with the following composition in weight percentages: 46.0 to 51.0% Cu, 8.0 to 11.0% Ni, 0.2 to 0.6% Mn, 0.05 to 0.5% Si, up to 0.8% of each of Fe and/or Co, the sum of the Fe content and double the Co content equaling at least 0.1 wt. %, residual Zn, and unavoidable impurities, wherein nickel-, iron-, and manganese-containing and/or nickel-, cobalt-, and manganese-containing mixed silicides are embedded into a microstructure consisting of α- and β-phases as spherical or ellipsoidal particles. The invention further relates to uses of a copper-nickel-zinc alloy according to the invention.
Opening claim text (preview).
1 . A copper-nickel-zinc alloy having the following composition [in % by weight]: Cu from 46.0 to 51.0%, Ni from 8.0 to 11.0%, Mn from 0.2 to 0.6%, Si from 0.05 to 0.5%, Fe and/or Co in each case up to 0.8%, where the sum of Fe content and twice the Co content is at least 0.1%, balance Zn and unavoidable impurities, wherein nickel-, iron- and manganese-containing and/or nickel-, cobalt- and manganese-containing mixed silicides are embedded as spherical or ellipsoidal particles in a microstructure consisting of α and β phase. 2 . The copper-nickel-zinc alloy as claimed in claim 1 having the following composition [in % by weight]: Cu from 47.5 to 49.5%, Ni from 8.0 to 10.0%, Mn from 0.2 to 0.6%, Si from 0.05 to 0.4%, Fe from 0.2 to 0.8%, optionally up to 0.8% of Co, balance Zn and unavoidable impurities, wherein nickel-, iron- and manganese-containing mixed silicides are embedded as spherical or ellipsoidal particles in a microstructure consisting of a and p phase. 3 . The copper-nickel-zinc alloy as claimed in claim 1 having the following composition [in % by weight]: Cu from 47.5 to 49.5%, Ni from 8.0 to 10.0%, Mn from 0.2 to 0.6%, Si from 0.05 to 0.4%, Co from 0.1 to 0.8%, optionally up to 0.8% of Fe, balance Zn and unavoidable impurities, wherein nickel-, cobalt- and manganese-containing mixed silicides are embedded as spherical or ellipsoidal particles in a microstructure consisting of α and β phase. 4 . The use of a copper-nickel-zinc alloy as claimed in claim 1 for producing consumer goods having demanding requirements in terms of the surface quality. 5 . The use of a copper-nickel-zinc alloy as claimed in claim 1 for producing keys, locks, plug connectors or points for ballpoint pens.
Related publications grouped by family.
Answers are generated from the same data shown on this page.