Glass laminate, and method for using block copolymer hydrogenation product as binder for glass laminate
US-2015104654-A1 · Apr 16, 2015 · US
US2018099486A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2018099486-A1 |
| Application number | US-201615567079-A |
| Country | US |
| Kind code | A1 |
| Filing date | Apr 14, 2016 |
| Priority date | Apr 22, 2015 |
| Publication date | Apr 12, 2018 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention is a laminated glass which is prepared by inserting a resin intermediate film between glass plates and adhering the glass plates to integrate them, having a bending deflection at 90° C. is 7.3 N/mm 2 or higher, a weight per unit area is 7.5 kg/m 2 or less, wherein the resin intermediate film contains a modified hydrogenated block copolymer [E] obtained by introducing an alkoxysilyl group into a hydrogenated block copolymer [D], storage elastic moduli in the dynamic viscoelastic properties of the resin intermediate film are 5×10 8 Pa or lower at a temperature of −20° C. and 2×10 7 Pa or higher at a temperature of 90° C., and the hydrogenated block copolymer [D] is obtained by hydrogenating 90% or more of carbon-carbon unsaturated bonds on a main chain and side chains and carbon-carbon unsaturated bonds on an aromatic ring in a specific block copolymer [C].
Opening claim text (preview).
1 . A laminated glass which is prepared by inserting a resin intermediate film between glass plates and adhering the glass plates to integrate them, having a bending deflection at 90° C. is 7.3 N/mm 2 or higher, a weight per unit area is 7.5 kg/m 2 or less, wherein the resin intermediate film contains a modified hydrogenated block copolymer [E] obtained by introducing an alkoxysilyl group into a hydrogenated block copolymer [D], storage elastic moduli in the dynamic viscoelastic properties of the resin intermediate film are 5×10 8 Pa or lower at a temperature of −20° C. and 2×10 7 Pa or higher at a temperature of 90° C., and the hydrogenated block copolymer [D] is obtained by hydrogenating 90% or more of carbon-carbon unsaturated bonds on a main chain and side chains and carbon-carbon unsaturated bonds on an aromatic ring in a block copolymer [C] which is containing at least two polymer blocks [A] mainly containing a structural unit derived from an aromatic vinyl compound and at least one polymer block [B] mainly containing a structural unit derived from an acyclic conjugated diene compound.
comprising polysiloxanes · CPC title
Impact strength, toughness · CPC title
Elastic · CPC title
3 layers · CPC title
Cars · CPC title