Window, display device including the same, and manufacturing method of window

US2018010010A1 · US · A1

Patent metadata
FieldValue
Publication numberUS-2018010010-A1
Application numberUS-201715617991-A
CountryUS
Kind codeA1
Filing dateJun 8, 2017
Priority dateJul 6, 2016
Publication dateJan 11, 2018
Grant date

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A window according to an exemplary embodiment of the present disclosure includes: a substrate; and a protective layer provided in one side of the substrate, wherein the protective layer includes at least one of a first compound represented as given in Chemical Formula 1 and a derivative thereof and at least one of a second compound represented as given in Chemical Formula 2 and a derivative thereof:

First claim

Opening claim text (preview).

What is claimed is: 1 . A window comprising: a substrate; and a protective layer on one side of the substrate, wherein the protective layer comprises at least one of a first compound represented as given in Chemical Formula 1 and a derivative thereof and at least one of a second compound represented as given Chemical Formula 2 and a derivative thereof: in Chemical Formula 1, R 1 denotes a C1 to C3 alkylene group or Chemical Formula 1-a, R 2 denotes a C1 to C3 alkyl group or Chemical Formula 1-b, and R 3 denotes a C1 to C3 alkyl group or Chemical Formula 1-c, in Chemical Formula 2, X denotes hydrogen or a methyl group, Y denotes —O— or —NH—, Z denotes —S— or —SO 2 —, R 7 and R 8 independently denote a substituted or unsubstituted C1 to C20 alkylene group, R 9 denotes a C1 to C12 fluoroalkyl group, and m denotes an integer between 0 and 2, inclusive, in Chemical Formula 1-a and Chemical Formula 1-b, R 4 denotes hydrogen or a C1 to C3 alkyl group, R 5 denotes a substituted or unsubstituted C1 to C30 alkylene group, and p denotes an integer between 1 and 10, inclusive, and in Chemical Formula 1-c, q denotes an integer between 1 and 10, inclusive. 2 . The window of claim 1 , wherein the protective layer comprises a first area and a second area, the first area is provided closer to the substrate than the second area, and the first area comprises a hard coating component, and the second area comprises an anti-fingerprint component. 3 . The window of claim 2 , wherein the hard coating component comprises at least one of the first compound and a derivative of the first compound, and the anti-fingerprint component comprises at least one of the second compound and a derivative of the second compound. 4 . The window of claim 2 , wherein a thickness of the second area is thinner than a thickness of the first area. 5 . The window of claim 1 , wherein in Chemical Formula 1-a and Chemical formula 1-b, R 5 is one selected from the group consisting of a methylene group, an ethylene group, a propylene group, an isopropylene group, an n-butylene group, an s-butylene group, an isobutylene group, a t-butylene group, an n-pentylene group, an n-hexylene group, an n-heptylene group, and an n-octylene group. 6 . The window of claim 1 , wherein, in Chemical Formula 2, R 7 and R 8 are each one selected from the group consisting of an methylene group, an ethylene group, a propylene group, an isopropylene group, an n-butylene group, an s-butylene group, an isobutylene group, a t-butylene group, an n-pentylene group, an n-hexylene group, an n-heptylene group, and an n-octylene group. 7 . The window of claim 1 , wherein pencil hardness of the protective window is greater than or equal to 1H and a contact angle is greater than or equal to 105 degrees. 8 . A display device comprising a window, wherein the window comprises a substrate; and a protective layer on one side of the substrate, wherein the protective layer comprises at least one of a first compound represented as given in Chemical Formula 1 and a derivative thereof and at least one of a second compound represented as given Chemical Formula 2 and a derivative thereof: in Chemical Formula 1, R1 denotes an a C1 to C3 alkylene group or Chemical Formula 1-a, R2 denotes a C1 to C3 alkyl group or Chemical Formula 1-b, and R3 denotes a C1 to C3 alkyl group or Chemical Formula 1-c, in Chemical Formula 2, X denotes hydrogen or a methyl group, Y denotes —O— or —NH—, Z denotes —S— or —SO 2 —, R7 and R8 independently denote a substituted or unsubstituted C1 to C20 alkylene group, R9 denotes a C1 to C12 fluoroalkyl group, and m denotes an integer between 0 and 2, inclusive, in Chemical Formula 1-a and Chemical Formula 1-b, R4 denotes hydrogen or a C1 to C3 alkyl group, R5 denotes a substituted or unsubstituted C1 to C30 alkylene group, and p denotes an integer between 1 and 10, inclusive, and in Chemical Formula 1-c, q denotes an integer between 1 and 10, inclusive. 9 . A method for manufacturing a window, comprising: coating a protective material on at least one side of a substrate; and forming a protective layer by curing the coated protective material, wherein the coating of the protective material uses a one-liquid type solution that includes a hard coating component and an anti-fingerprint component. 10 . The method for manufacturing the window of claim 9 , further comprising drying the protective layer before the curing of the protective material. 11 . The method for manufacturing the window of claim 10 , wherein the curing the protective material comprises irradiating ultraviolet rays to the substrate. 12 . The method for manufacturing the window of claim 9 , wherein the coating of the protective material comprises immersing the substrate in the one-liquid type solution. 13 . The method for manufacturing the window of claim 9 , wherein the hard coating component is a compound represented as given in Chemical Formula 1, and the anti-fingerprint component is a compound represented as given in Chemical Formula 2: in Chemical Formula 1, R 1 denotes a C1 to C3 alkylene group or Chemical Formula 1-a, R 2 denotes a C1 to C3 alkyl group or Chemical Formula 1-b, and R 3 denotes a C1 to C3 alkyl group or Chemical Formula 1-c, in Chemical Formula 2, X denotes hydrogen or a methyl group, Y denotes —O— or —NH—, Z denotes —S— or —SO 2 —, R 7 and R 8 independently denote a substituted or unsubstituted C1 to C20 alkyl group, R 9 denotes a C1 to C12 fluoroalkyl group, and m denotes an integer between 0 and 2, inclusive, in Chemical Formula 1-a and Chemical Formula 1-b, R 4 denotes hydrogen or a C1 to C3 alkyl group, R 5 denotes a substituted or unsubstituted C1 to C30 alkylene group, and p denotes an integer between 1 and 10, inclusive, and in Chemical Formula 1-c, q denotes an integer between 1 and 10, inclusive. 14 . The method for manufacturing the window of claim 13 , wherein in Chemical Formula 1-a and Chemical Formula 1-b, R 5 is one selected from the group consisting of a methylene group, an ethylene group, a propylene group, an isopropylene group, an n-butylene group, an s-butylene group, an isobutylene group, a t-butylene group, an n-pentylene group, an n-hexylene group, an n-heptylene group, and an n-octylene group. 15 . The method for manufacturing the window of claim 13 , wherein, in Chemical Formula 2, R 7 and R 8 are each one selected from the group consisting of an methylene group, an ethylene group, a propylene group, an isopropylene group, an n-butylene group, an s-butylene group, an isobutylene group, a t-butylene group, an n-pentylene group, an n-hexylene group, an n-heptylene group, and an n-octylene group. 16 . The method for manufacturing the window of claim 9 , wherein the one-liquid type solution comprises a polar solvent. 17 . The method for manufacturing the window

Assignees

Inventors

Classifications

  • C09D133/14Primary

    of esters containing halogen, nitrogen, sulfur or oxygen atoms in addition to the carboxy oxygen · CPC title

  • performed by dipping · CPC title

  • with means to keep optical surfaces clean, e.g. by preventing or removing dirt, stains, contamination, condensation (G02B1/18 takes precedence; cleaning in general B08B) · CPC title

  • Curing or cross-linking the coating · CPC title

  • Protective coatings, e.g. hard coatings · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US2018010010A1 cover?
A window according to an exemplary embodiment of the present disclosure includes: a substrate; and a protective layer provided in one side of the substrate, wherein the protective layer includes at least one of a first compound represented as given in Chemical Formula 1 and a derivative thereof and at least one of a second compound represented as given in Chemical Formula 2 and a derivative the…
Who is the assignee on this patent?
Samsung Display Co Ltd
What technology area does this patent fall under?
Primary CPC classification C09D133/14. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Thu Jan 11 2018 00:00:00 GMT+0000 (Coordinated Universal Time) (A1). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).